Category: | PP Homopolymer , Polypropylene Homopolymer |
Manufacturer: | Polykemi AB |
Trademark: | POLYfill |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | tmrE7P_POLYfill-PPH-GF20005-PD2-UV.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Glass fibre-reinforced Chemically coupled |
General Information | |
---|---|
Filler / Reinforcement |
|
Features |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.940 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 20 | g/10 min | ISO 1133 |
Molding Shrinkage | ISO 294-4 | ||
Across Flow | 0.90 to 1.2 | % | |
Flow | 0.40 to 0.70 | % |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | 44.0 | MPa | ISO 527-2 |
Tensile Strain | ISO 527-2 | ||
Yield | 7.8 | % | |
Break | 8.5 | % | |
Flexural Modulus (23°C) | 2400 | MPa | ISO 178 |
Flexural Stress | 70.0 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179 | ||
-20°C | 2.8 | kJ/m² | |
23°C | 5.0 | kJ/m² | |
Charpy Unnotched Impact Strength (23°C) | 32 | kJ/m² | ISO 179 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature 1 | |||
0.45 MPa, Unannealed | 150 | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 75.0 | °C | ISO 75-2/A |
Vicat Softening Temperature | |||
-- | 107 | °C | ISO 306/A50 |
-- | 110 | °C | ISO 306/B50 |
Note Message | |
---|---|
1 . | 120°C/hr |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Cellophane™ CelloPlus™ W (White) | Innovia Films Ltd. | Cellulose, Regenerated | Cellophane™ |
Fainplast PVC GS 4510/R | Fainplast Compounds S.r.l | PVC, Unspecified | Fainplast PVC |
Greenflex® ML 50 F | Versalis S.p.A. | EVA | Greenflex® |
KOCETAL® MS301S | Kolon Plastics, Inc. | Acetal (POM) Copolymer | KOCETAL® |
SQUARE® LSR6900-15A/B | Shenzhen SQUARE Silicone Co., Ltd. | Silicone Rubber, LSR | SQUARE® |