| Category: | Nylon 66 , Polyamide 66 |
| Manufacturer: | Wellman Engineering Resins |
| Trademark: | Wellamid® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | t9m3qT_Wellamid-GF33-66-22LH-NBK1.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Wellamid® GF33-66 22LH-NBK1 is a Polyamide 66 (Nylon 66) material filled with 33% glass fiber. It is available in Asia Pacific, Europe, Latin America, or North America. Typical application of Wellamid® GF33-66 22LH-NBK1: Automotive |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Uses |
|
| Appearance |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.40 | g/cm³ | ISO 1183 |
| Molding Shrinkage | ISO 294-4 | ||
| Across Flow : 23°C | 1.1 to 1.5 | % | |
| Flow : 23°C | 0.20 to 0.60 | % |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Yield, 23°C) | 165 | MPa | ISO 527-2 |
| Tensile Strain (Yield, 23°C) | 2.0 | % | ISO 527-2 |
| Flexural Modulus (23°C) | 9600 | MPa | ISO 178 |
| Flexural Stress (23°C) | 240 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength (23°C) | 7.0 | kJ/m² | ISO 180 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 240 | °C | ISO 75-2/A |
| Melting Temperature (DSC) | 260 | °C | ISO 3146 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| CompaDur® 121 GF 30 LW natural (007) | DimeLika Plast GmbH | PBT | CompaDur® |
| FORMULA P COMP 5220 M1 | Putsch Kunststoffe GmbH | PP, Unspecified | FORMULA P |
| Hanwha Total PE 310A | HANWHA TOTAL PETROCHEMICALS Co., Ltd. | LDPE | Hanwha Total PE |
| Huaxia Shenzhou PFA DS700 | Shandong Huaxia Shenzhou New Material Co., Ltd. | PFA | Huaxia Shenzhou |
| POLYCOMPO PP J136 | POLYCOMPO Co.,Ltd. | PP, Unspecified | POLYCOMPO PP |