TECHNYL® C 236SI V30 Natural is a polyamide 6 reinforced with 30% of glass fiber, with improved impact resistance, for injection moulding. This grade offers high impact strength and good mechanical properties. |
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Uses |
|
Agency Ratings |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Resin ID (ISO 1043) |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.34 | -- | g/cm³ | ISO 1183/A |
Water Absorption (23°C, 24 hr) | 0.93 | -- | % | ISO 62 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus (23°C) | 9500 | 5200 | MPa | ISO 527-2/1A |
Tensile Stress (Break, 23°C) | 150 | 95.0 | MPa | ISO 527-2/1A |
Tensile Strain (Break, 23°C) | 4.0 | -- | % | ISO 527-2 |
Flexural Modulus (23°C) | 7600 | 4000 | MPa | ISO 178 |
Flexural Stress (23°C) | 227 | -- | MPa | ISO 178 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | |||
-30°C | 13 | -- | kJ/m² | ISO 179/1eA |
23°C | 18 | 32 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength | ISO 179/1eU | |||
-30°C | 98 | 98 | kJ/m² | ISO 179/1eU |
23°C | 92 | 100 | kJ/m² | ISO 179/1eU |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 205 | -- | °C | ISO 75-2/Af |
Melting Temperature | 222 | -- | °C | ISO 11357-3 |
Injection | Dry | Unit | |
---|---|---|---|
Drying Temperature | 80 | °C | |
Suggested Max Moisture | 0.080 | % | |
Rear Temperature | 250 - 270 | °C | |
Middle Temperature | 260 - 280 | °C | |
Front Temperature | 260 - 290 | °C | |
Mold Temperature | 70 - 90 | °C |
Injection instructions |
---|
The material is supplied in airtight bags, ready for use. In case that the virgin material has absorbed moisture, it must be dried with a dehumidified air drying equipment, dew point mini -20°C. Recommended time 2-4hInjection Advice: For reinforced polyamide, Solvay recommends the use of steel with a high content of Carbon and purified for polishing to avoid or limit the abrasion. For example: X38CrMoV5-1 (EN Norm) - 1.2367 /1.2343 (DIN Norm) or X160CrMoV12 (EN Norm) - 1.2601 /1.2379 (DIN Norm). For Mould Temperature, in the case of parts where the surface roughness is required we can recommend a temperature of 90°C to 120°C with an optimum at 105°C. |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Makrolon® LQ3187 | Covestro - Polycarbonates | PC | Makrolon® |
APEX® 1560 | Teknor Apex Company | PVC, Flexible | APEX® |
IDI BMC B30 (Glass Content 25%) | IDI Composites International | TS, Unspecified | IDI BMC |
Plaslube® PC CF15 TL6 BK | Techmer Engineered Solutions | PC | Plaslube® |
POCAN® KU 2-7503/1 000000 | LANXESS GmbH | PBT | POCAN® |