| Category: | PUR-Ester/TDI , Polyurethane (Polyester, TDI) |
| Manufacturer: | Anderson Development Company |
| Trademark: | Andur |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | smYrzW_Andur-9-AP-Curene-442.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| All properties based on Andur® 9-AP cured with Curene® 442 |
| General Information | |
|---|---|
| Forms |
|
| Processing Method |
|
| Hardness | Nominal Value | Test Method | |
|---|---|---|---|
| Durometer Hardness (Shore A) | 90 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength | 46.2 | MPa | ASTM D638 |
| Tensile Elongation (Break) | 600 | % | ASTM D638 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ASTM D412 | ||
| 100% strain | 5.52 | MPa | ASTM D412 |
| 300% strain | 18.6 | MPa | ASTM D412 |
| Tear Strength 1 | 101 | kN/m | ASTM D624 |
| Compression Set | 28 | % | ASTM D395 |
| Thermoset | Nominal Value | Unit | |
|---|---|---|---|
| Pot Life | 7.0 - 8.0 | min | |
| Demold Time | 30 - 40 | min |
| Additional Information |
|---|
| Hardness, Shore A: 90-92Curene® 442 Temperature, °F: 240-250Prepolymer Temperature, °F: 212-220 |
| Note Message | |
|---|---|
| 1 . | C mould |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 903 TFE 15 Z | RTP Company | PSU | RTP |
| Rotec® ABS SE 3 HH | ROMIRA GmbH | ABS | Rotec® ABS |
| Ultramid® B3ZG3 | BASF Corporation | Nylon 6 | Ultramid® |
| CABELEC® CA0887 | Cabot Corporation | EVA | CABELEC® |
| Grilamid® 1SBVX-30H LDS black | EMS-GRIVORY | Nylon 1010 | Grilamid® |