RTP 2205 LF

Category: PEEK , Polyetheretherketone
Manufacturer: RTP Company
Trademark: RTP
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: shQ223_RTP-2205-LF.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Glass Fiber - Low Flow
General Information
Filler / Reinforcement
  • Glass fiber reinforced material, 30% filler by weight
Features
  • Low liquidity
RoHS Compliance
  • Contact manufacturer
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.52g/cm³ASTM D792
Molding Shrinkage - Flow (3.20 mm)0.30%ASTM D955
Moisture Content 0.10%
Additional InformationNominal ValueUnit
Primary Additive 30%
MechanicalNominal ValueUnitTest Method
Tensile Modulus 11700MPaASTM D638
Tensile Strength 172MPaASTM D638
Tensile Elongation (Yield)2.5%ASTM D638
Flexural Modulus 11000MPaASTM D790
Flexural Strength 255MPaASTM D790
ImpactNominal ValueUnitTest Method
Notched Izod Impact (3.20 mm)120J/mASTM D256
Unnotched Izod Impact (3.20 mm)910J/mASTM D4812
ThermalNominal ValueUnitTest Method
Deflection Temperature Under Load (1.8 MPa, Unannealed)316°CASTM D648
FlammabilityNominal ValueTest Method
Flame Rating (1.50 mm, ** Values per RTP Company testing.)V-0UL 94
InjectionNominal ValueUnit
Drying Temperature 149°C
Drying Time 3.0hr
Dew Point -28.9°C
Processing (Melt) Temp 349 - 399°C
Mold Temperature 163 - 218°C
Injection Pressure 82.7 - 124MPa
Injection instructions
Desiccant Type Dryer Required.
Resin Grade Manufacturer Category Trademark
VESTAKEEP® 2000UFP20 Evonik Industries AG PEEK VESTAKEEP®
BioSpan® SPU DSM Biomedical Inc. PUR, Unspecified BioSpan®
Elvaloy® AC 2618 DuPont Packaging & Industrial Polymers EEA Elvaloy®
LOXIM 300 00 V0 LOXIM Industries Private Limited Nylon 6 LOXIM
MAJORIS ET261 - 7798 AD majoris PP, Unspecified MAJORIS