ALTECH® PA6 B 1000/209

Category: Nylon 6 , Polyamide 6
Manufacturer: ALBIS PLASTIC GmbH
Trademark: ALTECH® PA6
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: sc4LA5_ALTECH-PA6-B-1000-209.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
ALTECH® PA6 B 1000/209 is a Polyamide 6 (Nylon 6) product. It is available in Asia Pacific, Europe, or North America.

Characteristics include:
  • REACH Compliant
  • RoHS Compliant
  • Good Mold Release
General Information
Features
  • Good Mold Release
Agency Ratings
  • EC 1907/2006 (REACH)
RoHS Compliance
  • RoHS Compliant
PhysicalDryConditionedUnitTest Method
Density 1.13--g/cm³ISO 1183
Water Absorption ISO 62
     Saturation, 23°C 9.5--%
     Equilibrium, 23°C, 50% RH 2.9--%
MechanicalDryConditionedUnitTest Method
Tensile Modulus 3300--MPaISO 527-2
Tensile Stress 60.0--MPaISO 527-2
Tensile Strain (Break)9.0--%ISO 527-2
Flexural Modulus 2700--MPaISO 178
Flexural Stress 105--MPaISO 178
ImpactDryConditionedUnitTest Method
Charpy Notched Impact Strength 5.5--kJ/m²ISO 179/1eA
Charpy Unnotched Impact Strength 550--kJ/m²ISO 179/1eU
ThermalDryConditionedUnitTest Method
Heat Deflection Temperature (1.8 MPa, Unannealed)66.0--°CISO 75-2/A
ElectricalDryConditionedUnitTest Method
Surface Resistivity --1.0E+12ohmsIEC 60093
Volume Resistivity 1.0E+14--ohms·cmIEC 60093
Comparative Tracking Index 550--VIEC 60112
InjectionDryUnit
Drying Temperature - Desiccant Dryer 80.0°C
Drying Time - Desiccant Dryer 2.0 to 12hr
Suggested Max Moisture 0.15%
Processing (Melt) Temp 250 to 270°C
Mold Temperature 40.0 to 80.0°C
Resin Grade Manufacturer Category Trademark
Spartech Polycom X03831 Spartech Polycom PP Homopolymer Spartech
NEXUS PP HPP30 Nexus Resin Group, LLC. PP Homopolymer NEXUS PP
Baoding 67I85 Baoding Bangtai Polymeric New-Materials Co.,Ltd TPU-Polyester Baoding