| TECHNYL® A 118 V50 Black 21 is a polyamide 66, reinforced with 50% of glass fibre, heat stabilized and modified viscosity, for injection moulding. This grade offers excellent combination between thermal and mechanical properties. It has a high fluency that permits the injection mould of big dimension or complex geometric structures, an excellent dimensional stability and chemical stability. |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Additive |
|
| Features |
|
| RoHS Compliance |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Multi-Point Data |
|
| Resin ID (ISO 1043) |
|
| Physical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Density | 1.55 | -- | g/cm³ | ISO 1183/A |
| Water Absorption | ISO 62 | |||
| 23°C, 24 hr | 0.60 | -- | % | ISO 62 |
| Saturated, 23°C | 3.6 | -- | % | ISO 62 |
| Equilibrium, 23°C, 50% RH | 1.4 | -- | % | ISO 62 |
| Mechanical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Tensile Modulus (23°C) | 17000 | 13600 | MPa | ISO 527-2/1A |
| Tensile Stress (Break, 23°C) | 215 | 155 | MPa | ISO 527-2/1A |
| Tensile Strain (Break, 23°C) | 2.2 | 3.2 | % | ISO 527-2 |
| Impact | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Charpy Notched Impact Strength (23°C) | 14 | 15 | kJ/m² | ISO 179/1eA |
| Charpy Unnotched Impact Strength | ||||
| 23°C | 80 | 75 | kJ/m² | ISO 179/1eU |
| 23°C | 90 | -- | kJ/m² | ISO 179/1fU |
| Notched Izod Impact (23°C) | 14 | 16 | kJ/m² | ISO 180 |
| Thermal | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 250 | -- | °C | ISO 75-2/Af |
| Melting Temperature | 261 | -- | °C | ISO 11357-3 |
| Injection | Dry | Unit | |
|---|---|---|---|
| Drying Temperature | 80 | °C | |
| Suggested Max Moisture | 0.20 | % | |
| Rear Temperature | 270 - 280 | °C | |
| Middle Temperature | 280 - 290 | °C | |
| Front Temperature | 280 - 300 | °C | |
| Mold Temperature | 70 - 100 | °C |
| Injection instructions |
|---|
| The material is supplied in airtight bags, ready for use. In case that the virgin material has absorbed moisture, it must be dried with a dehumidified air drying equipment, dew point mini -20°C. Recommended time 2-4hInjection Advice: For reinforced polyamide, Solvay recommends the use of steel with a high content of Carbon and purified for polishing to avoid or limit the abrasion. For example: X38CrMoV5-1 (EN Norm) - 1.2367 /1.2343 (DIN Norm) or X160CrMoV12 (EN Norm) - 1.2601 /1.2379 (DIN Norm). For Mould Temperature, in the case of parts where the surface roughness is required we can recommend a temperature of 90°C to 120°C with an optimum at 105°C. The processing parameters like processing temperatures are a recommendation and can be adjusted in function of injection machine size, part geometry / design |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Razalen® R113-01 | Razin™ Engineering Plastics | PP, Unspecified | Razalen® |
| SLOVALEN® PH 51 N | Plastcom | PP, Unspecified | SLOVALEN® |
| BP RPP 2012 TR BLK | Buckeye Polymers, Inc. | PP, Unspecified | BP |
| PETILEN S 23/59 | PETKIM Petrokimya Holding A.S. | PVC, Rigid | PETILEN |
| Plaslube® ABS TL2 | Techmer Engineered Solutions | ABS | Plaslube® |