Category: | Nylon 6 , Polyamide 6 |
Manufacturer: | EMS-GRIVORY |
Trademark: | Grilon® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | rx6hX1_Grilon-BGM-65-X-V0.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Grilon® BGM-65 X V0 is a Polyamide 6 (Nylon 6) material filled with 65% glass\mineral. It is available in Africa & Middle East, Asia Pacific, Europe, Latin America, or North America for injection molding. Important attributes of Grilon® BGM-65 X V0 are:
Typical applications include:
|
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Uses |
|
RoHS Compliance |
|
Forms |
|
Processing Method |
|
Multi-Point Data |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.69 | -- | g/cm³ | ISO 1183 |
Molding Shrinkage | ISO 294-4 | |||
Across Flow | 0.60 | -- | % | |
Flow | 0.20 | -- | % | |
Water Absorption | ISO 62 | |||
Saturation, 23°C | 5.0 | -- | % | |
Equilibrium, 23°C, 50% RH | 1.5 | -- | % |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus | 11500 | 7100 | MPa | ISO 527-2 |
Tensile Stress (Break) | 120 | 90.0 | MPa | ISO 527-2 |
Tensile Strain (Break) | 1.0 | 3.0 | % | ISO 527-2 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | |||
-30°C | 3.0 | 3.0 | kJ/m² | |
23°C | 3.0 | 3.0 | kJ/m² | |
Charpy Unnotched Impact Strength | ISO 179/1eU | |||
-30°C | 15 | 15 | kJ/m² | |
23°C | 25 | 25 | kJ/m² |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature | ||||
0.45 MPa, Unannealed | 75.0 | -- | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 160 | -- | °C | ISO 75-2/A |
Continuous Use Temperature | Internal Method | |||
-- 1 | 80.0 to 110 | -- | °C | |
-- 2 | 160 | -- | °C | |
Melting Temperature 3 | 222 | -- | °C | ISO 11357-3 |
CLTE | ISO 11359-2 | |||
Flow | 3.0E-5 | -- | cm/cm/°C | |
Transverse | 6.0E-5 | -- | cm/cm/°C |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Surface Resistivity | -- | 1.0E+12 | ohms | IEC 60093 |
Volume Resistivity | 1.0E+14 | 1.0E+13 | ohms·cm | IEC 60093 |
Electric Strength | 33 | 29 | kV/mm | IEC 60243-1 |
Relative Permittivity (100 Hz) | 3.00 | 3.00 | IEC 60250 | |
Dissipation Factor (100 Hz) | 1.0E-3 | 1.0E-3 | IEC 60250 | |
Comparative Tracking Index | -- | 500 | V | IEC 60112 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Flammability Classification | IEC 60695-11-10, -20 | |||
1.50 mm | V-0 | -- | ||
3.00 mm | V-0 | -- | ||
Oxygen Index | 65 | -- | % | ISO 4589-2 |
Additional Information | Dry | Conditioned | Test Method | |
---|---|---|---|---|
ISO Type | PA6, MFHR, 14-110, (MD+GF)65 X | -- | ISO 1874 |
Note Message | |
---|---|
1 . | Long Term |
2 . | Short Term |
3 . | 10°C/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
TECHNYL® A 216 V30 NATURAL | Solvay Engineering Plastics | Nylon 66 | TECHNYL® A |
NEXUS PP HPP30 | Nexus Resin Group, LLC. | PP Homopolymer | NEXUS PP |
Delta N66R-1M80 | Delta Polymers | Nylon 66 | Delta |
Elastollan® 1185A10V | BASF Corp. Thermoplastic Polyurethanes | TPU-Polyether | Elastollan® |
LUVOCOM® 1105-8001 VP | Lehmann & Voss & Co. | PEEK | LUVOCOM® |