Category: | SEBS , Styrene Ethylene Butylene Styrene Block Copolymer |
Manufacturer: | Teknor Apex Company |
Trademark: | Elexar® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | rgS3cU_Elexar-EL-1934F.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Elexar®EL-1934F is a styrene-ethylene-butylene-styrene block copolymer (SEBS) material,. This product is available in North America, Africa and the Middle East, Latin America, Europe or Asia Pacific. The processing method is extrusion or injection molding. Elexar®The main features of the EL-1934F are:
Typical application areas include:
|
General Information | |
---|---|
Features |
|
Uses |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.30 | g/cm³ | ASTM D792 |
Melt Mass-Flow Rate (MFR) (200°C/5.0 kg) | 31 | g/10 min | ASTM D1238 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A) | 70 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength (Break) | 9.65 | MPa | ASTM D412 |
Tensile Elongation (Break) | 600 | % | ASTM D412 |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Change in Tensile Strength in Air (136°C, 168 hr) | 5.0 | % | ASTM D573 |
Change in Ultimate Elongation in Air (136°C, 168 hr) | -2.0 | % | ASTM D573 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Continuous Use Temperature | 105 | °C | UL 1581 |
Brittleness Temperature | < -60.0 | °C | ASTM D746 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Dielectric Strength | 38 | kV/mm | ASTM D149 |
Dielectric Constant | 2.50 | ASTM D150 | |
Dissipation Factor | 3.0E-3 | ASTM D150 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating (1.52 mm) | V-0 | UL 94 | |
Oxygen Index | 31 | % | ASTM D2863 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Rear Temperature | 199 - 216 | °C | |
Middle Temperature | 213 - 221 | °C | |
Front Temperature | 221 - 227 | °C | |
Nozzle Temperature | 221 - 229 | °C | |
Processing (Melt) Temp | 221 - 229 | °C | |
Mold Temperature | 25.0 - 65.6 | °C | |
Injection Pressure | 1.38 - 6.89 | MPa | |
Injection Rate | Moderate-Fast | ||
Back Pressure | 0.172 - 0.345 | MPa | |
Screw Speed | 50 - 100 | rpm | |
Cushion | 3.81 - 25.4 | mm |
Injection instructions |
---|
无需干燥。但如果湿度过大,则将粒料在150°F (65°C)的温度下干燥2-4小时。 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Cylinder Zone 1 Temp. | 193 - 210 | °C | |
Cylinder Zone 2 Temp. | 199 - 216 | °C | |
Cylinder Zone 3 Temp. | 213 - 221 | °C | |
Cylinder Zone 5 Temp. | 221 - 227 | °C | |
Die Temperature | 221 - 229 | °C |
Extrusion instructions |
---|
螺杆转速30 - 100 rpm |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Adflex X 100 G | LyondellBasell Industries | TPO (POE) | Adflex |
FHR Polypropylene 23H2A | Flint Hills Resources, LP | PP Random Copolymer | FHR Polypropylene |
LNP™ THERMOCOMP™ 2Z004 compound | SABIC Innovative Plastics | ETFE | LNP™ THERMOCOMP™ |
Hostacom HBG 479R BLACK | LyondellBasell Industries | PP Homopolymer | Hostacom |
Sylvin 8200-88 Blue 8420 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |