| Category: | Nylon 6 , Polyamide 6 |
| Manufacturer: | Shakespeare Monofilaments and Specialty Polymers |
| Trademark: | Isocor™ |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | rgGugG_Isocor-637.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Isocor™ 637 multi-polymer is a linear polyamide with unique solubility characteristics and physical properties. Unlike conventional polyamides, Isocor™ 637 is soluble in common alcohols or in alcohol / water mixtures. Isocor™ 637 is easily processed and has a wide range of applications due to its physical properties, chemical resistance, and lower melt temperatures. Typical applications for Isocor™ 637 include:
|
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.07 | g/cm³ | ASTM D792 |
| Water Absorption (24 hr) | 3.5 | % | ASTM D570 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore D) | 62 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength (Yield) | 47.6 | MPa | ASTM D638 |
| Tensile Elongation (Break) | 360 | % | ASTM D638 |
| Flexural Modulus | 179 | MPa | ASTM D790 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Melting Temperature | 145 | °C | DSC |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Volume Resistivity | 1.0E+12 | ohms·cm | ASTM D257 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Dew Point | < -17.8 | °C | |
| Suggested Max Moisture | 0.20 | % | |
| Hopper Temperature | 60.0 | °C | |
| Rear Temperature | 143 - 154 | °C | |
| Middle Temperature | 149 - 160 | °C | |
| Front Temperature | 154 - 166 | °C | |
| Nozzle Temperature | 143 - 154 | °C | |
| Processing (Melt) Temp | 143 - 154 | °C | |
| Mold Temperature | 10.0 - 93.3 | °C | |
| Injection Pressure | 3.45 - 13.8 | MPa | |
| Injection Rate | Fast | ||
| Back Pressure | 0.689 | MPa |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Suggested Max Moisture | 0.10 | % | |
| Hopper Temperature | 79.4 | °C | |
| Cylinder Zone 1 Temp. | 218 | °C | |
| Cylinder Zone 2 Temp. | 246 | °C | |
| Cylinder Zone 3 Temp. | 246 | °C | |
| Cylinder Zone 4 Temp. | 246 | °C | |
| Die Temperature | 229 | °C |
| Extrusion instructions |
|---|
| Flange: 445°F (229°C)Air Dew Point (max): 0°F (-18°C)Neck: 445°F (229°C)Head: 445°F (229°C)Pump: 445°F (229°C) |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 285 HS | RTP Company | Nylon 66 | RTP |
| TUFNYL® SXXIC SILVER GREY | SRF Ltd. | Nylon 6 | TUFNYL® |
| KYOCERA CT4200H | KYOCERA Chemical Corporation | PI, TS | KYOCERA |
| POLYFLAM® RMMB 40400 | A. Schulman Europe | PC+ABS | POLYFLAM® |
| Sylvin 7868-75C Black | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |