| Category: | TPV , Thermoplastic Vulcanizate |
| Manufacturer: | Elastron USA, Inc. |
| Trademark: | Elastron® V |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | rPR9TD_Elastron-V-V101-A60-B.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
A soft, black thermoplastic vulcanizate, TPV (EPDM/PP) in the thermoplastic elastomer family that offers good physical properties and chemical resistance. Bondable to: PP, EVA, PE |
| General Information | |
|---|---|
| Features |
|
| RoHS Compliance |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 0.970 | g/cm³ | ASTM D792 |
| Molding Shrinkage | ASTM D955 | ||
| Flow | 2.7 | % | |
| Across Flow | 0.93 | % |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A) | 60 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Abrasion | 160 | mm³ | ASTM D1630 |
| Additional Information | Nominal Value | Test Method | |
|---|---|---|---|
| Ozone Resistance - Stressed | No Cracks | ASTM D518 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ASTM D412 | ||
| 100% Strain | 1.90 | MPa | |
| 300% Strain | 3.80 | MPa | |
| Tensile Strength (Break) | 5.50 | MPa | ASTM D412 |
| Tensile Elongation (Break) | 600 | % | ASTM D412 |
| Tear Strength | 31.0 | kN/m | ASTM D624 |
| Compression Set | ASTM D395 | ||
| 23°C, 22 hr | 17 | % | |
| 70°C, 22 hr | 33 | % | |
| 100°C, 22 hr | 46 | % |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 90.0 | °C | |
| Drying Time | 2.0 | hr | |
| Suggested Max Regrind | 20 | % | |
| Rear Temperature | 155 to 175 | °C | |
| Middle Temperature | 165 to 185 | °C | |
| Front Temperature | 170 to 190 | °C | |
| Nozzle Temperature | 180 to 210 | °C | |
| Mold Temperature | 25.0 to 50.0 | °C |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 90.0 | °C | |
| Drying Time | 2.0 | hr | |
| Cylinder Zone 1 Temp. | 155 to 165 | °C | |
| Cylinder Zone 2 Temp. | 160 to 180 | °C | |
| Cylinder Zone 3 Temp. | 165 to 185 | °C | |
| Cylinder Zone 4 Temp. | 170 to 190 | °C | |
| Cylinder Zone 5 Temp. | 180 to 210 | °C | |
| Die Temperature | 185 to 215 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Sylvin 90680-60 BLACK | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
| ETILINAS LL0209AA | POLYETHYLENE MALAYSIA SDN BHD | LLDPE | ETILINAS |
| HiFill® PC / PET 2230 HF UV | Techmer Engineered Solutions | PC+PBT | HiFill® |
| KOPLA PA66 KDP1000F | KOPLA Co., Ltd. | Nylon 66 | KOPLA PA66 |
| Tunhe PET TH106 | Xinjiang Blueridge Tunhe Chemical Industry Co.,Ltd | PET | Tunhe PET |