Category: | Nylon 66 , Polyamide 66 |
Manufacturer: | EPIC Polymers |
Trademark: | Strator® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | rMewMM_STRATOR-A-4.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
STRATOR® A-4 is a Polyamide 66 (Nylon 66) product filled with 40% long glass fiber. It is available in Europe. |
General Information | |
---|---|
Filler / Reinforcement |
|
Forms |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.50 | -- | g/cm³ | ISO 1183 |
Molding Shrinkage - Flow | 0.30 | -- | % | ISO 294-4 |
Water Absorption (Equilibrium, 23°C, 50% RH) | 1.5 | -- | % | ISO 62 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus | ISO 527-2 | |||
23°C | 13600 | 10200 | MPa | |
90°C | 8900 | -- | MPa | |
120°C | 7900 | -- | MPa | |
Tensile Stress | ISO 527-2 | |||
Yield, 23°C | 220 | 190 | MPa | |
Yield, 90°C | 140 | -- | MPa | |
Yield, 120°C | 120 | -- | MPa | |
Tensile Strain (Break, 23°C) | 2.6 | -- | % | ISO 527-2 |
Flexural Modulus (23°C) | 12000 | 9100 | MPa | ISO 178 |
Flexural Stress (23°C) | 330 | 270 | MPa | ISO 178 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength (23°C) | 30 | 35 | kJ/m² | ISO 179 |
Charpy Unnotched Impact Strength (23°C) | 70 | 90 | kJ/m² | ISO 179 |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature | ||||
0.45 MPa, Unannealed | 255 | -- | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 250 | -- | °C | ISO 75-2/A |
CLTE - Flow (23°C) | 2.3E-5 | -- | cm/cm/°C | ISO 7991 |
Thermal Conductivity | 0.33 | -- | W/m/K | ISO 22007 |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Surface Resistivity | 1.0E+12 | -- | ohms | ASTM D257 |
Electric Strength | 35 | -- | kV/mm | IEC 60243-1 |
Comparative Tracking Index | 500 | -- | V | IEC 60112 |
Injection | Dry | Unit | |
---|---|---|---|
Drying Temperature | 110 | °C | |
Drying Time | 4.0 | hr | |
Suggested Max Moisture | 0.10 | % | |
Rear Temperature | 270 to 300 | °C | |
Middle Temperature | 270 to 300 | °C | |
Front Temperature | 285 to 310 | °C | |
Nozzle Temperature | 285 to 320 | °C | |
Processing (Melt) Temp | < 310 | °C | |
Mold Temperature | 80.0 to 160 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Selvol™ 823 | Sekisui Chemical Company, Ltd. | PVOH | Selvol™ |
SITRALIN 21E / C6PS soul | SITRAPLAS GmbH | ASA+Nylon | SITRALIN |
Westlake LDPE EC477AA | Westlake Chemical Corporation | LDPE | Westlake LDPE |
Hytrel® HTR8341C BK320 | DuPont Performance Polymers | TPC-ET | Hytrel® |
Pebax® 4033 SA 01 MED | Arkema | PEBA-Ether | Pebax® |