| Category: | PBT , Polybutylene Terephthalate |
| Manufacturer: | RTP Company |
| Trademark: | RTP |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | quDvoH_RTP-1001-GB-15-TFE-5.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Glass Fiber - Glass Bead - PTFE Lubricated |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Additive |
|
| Features |
|
| RoHS Compliance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.51 | g/cm³ | ASTM D792 |
| Molding Shrinkage - Flow (3.20 mm) | 0.60 - 1.1 | % | ASTM D955 |
| Moisture Content | 0.030 | % |
| Additional Information | Nominal Value | Unit | |
|---|---|---|---|
| Primary Additive | 10 | % |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 5170 | MPa | ASTM D638 |
| Tensile Strength | 68.9 | MPa | ASTM D638 |
| Tensile Elongation (Yield) | 3.5 - 5.0 | % | ASTM D638 |
| Flexural Modulus | 4830 | MPa | ASTM D790 |
| Flexural Strength | 117 | MPa | ASTM D790 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact (3.20 mm) | 53 | J/m | ASTM D256 |
| Unnotched Izod Impact (3.20 mm) | 430 | J/m | ASTM D4812 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Deflection Temperature Under Load (1.8 MPa, Unannealed) | 79.4 | °C | ASTM D648 |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Volume Resistivity | 1.0E+14 - 1.0E+16 | ohms·cm | ASTM D257 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flame Rating (1.50 mm, ** Values per RTP Company testing.) | HB | UL 94 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 121 | °C | |
| Drying Time | 4.0 | hr | |
| Dew Point | -28.9 | °C | |
| Processing (Melt) Temp | 238 - 271 | °C | |
| Mold Temperature | 79.4 - 107 | °C | |
| Injection Pressure | 68.9 - 103 | MPa |
| Injection instructions |
|---|
| Desiccant Type Dryer Required. |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Reslen PPH 40K | Polimarky Spolka Jawna | PP Homopolymer | Reslen |
| Tarnoform® 300 AR | Grupa Azoty S.A. | Acetal (POM) Copolymer | Tarnoform® |
| Greenflex® ML 50 F | Versalis S.p.A. | EVA | Greenflex® |
| LNP™ VERTON™ RX10409D compound | SABIC Innovative Plastics | Nylon 66 | LNP™ VERTON™ |
| Sylvin 8687-55 Green 3159 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |