Polyamide 66, %25 glass fiber reinforced, V0 flammability |
General Information | |
---|---|
Filler / Reinforcement |
|
Recycled Content |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.27 to 1.32 | g/cm³ | ISO 1183 |
Molding Shrinkage | 0.45 to 0.60 | % |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Shore Hardness (Shore D) | 75 to 85 | ISO 868 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 5000 to 8000 | MPa | ISO 527-2 |
Tensile Stress (Yield) | 100 to 140 | MPa | ISO 527-2 |
Tensile Strain (Break) | > 5.0 | % | ISO 527-2 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact Strength | > 12 | kJ/m² | ISO 180/1A |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 245 | °C | ISO 75-2/A |
Vicat Softening Temperature | 255 | °C | ISO 306/B |
Melting Temperature (DSC) | 265 | °C | ISO 3146 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating | V-0 | UL 94 | |
Glow Wire Ignition Temperature | 960 | °C | VDE 0471/2 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Spartech Polycom SC5-4420 | Spartech Polycom | PP Copolymer | Spartech |
XANTAR® C CM 206 | Mitsubishi Engineering-Plastics Corp | PC+ABS | XANTAR® C |
Grilon® TSG-30/4 FA | EMS-GRIVORY | Nylon 66/6 | Grilon® |
LNP™ THERMOCOMP™ SF006 compound | SABIC Innovative Plastics | Nylon 12 | LNP™ THERMOCOMP™ |
Sylvin 9600-55 Clear | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |