| Category: | TPO (POE) , Thermoplastic Polyolefin Elastomer |
| Manufacturer: | LyondellBasell Industries |
| Trademark: | SEQUEL® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | qnGgbZ_SEQUEL-2326.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Sequel 2326 thermoplastic polyolefin material is designed for molded-in-color automotive interior applications that require energy-management properties. This product is typically supplied in natural or an OEM matched interior color with UV protection. Typical Customer Applications: Interior Applications |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Features |
|
| Uses |
|
| Appearance |
|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.960 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 15 | g/10 min | ISO 1133 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress 1(Yield) | 16.0 | MPa | ISO 527-2/50 |
| Flexural Modulus (23°C, 4.00 mm) | 1100 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact | ISO 180 | ||
| -40°C | 6.0 | kJ/m² | ISO 180 |
| 23°C | No Break | ISO 180 | |
| Instrumented Dart Impact 2 | ASTM D3763 | ||
| -30°C | 24.0 | J | ASTM D3763 |
| 23°C | 18.0 | J | ASTM D3763 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature | |||
| 0.45 MPa, not annealed | 75.0 | °C | ISO 75-2/B |
| 1.8 MPa, not annealed | 54.0 | °C | ISO 75-2/A |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 50.0 - 80.0 | °C | |
| Drying Time | 2.0 - 6.0 | hr | |
| Suggested Max Moisture | 0.050 | % | |
| Rear Temperature | 205 | °C | |
| Middle Temperature | 210 | °C | |
| Front Temperature | 215 | °C | |
| Nozzle Temperature | 215 | °C | |
| Processing (Melt) Temp | 190 - 240 | °C | |
| Mold Temperature | 30.0 | °C | |
| Injection Pressure | 3.50 - 10.5 | MPa | |
| Back Pressure | 0.350 - 2.00 | MPa | |
| Screw Speed | 50 - 100 | rpm | |
| Cushion | 6.00 - 13.0 | mm |
| Injection instructions |
|---|
| Hot Runner Manifold and Tips: 215°CMold Cavity Temperature: 30°CMold Core Temperature: 24°CInjection Pressure, High (first stage): 35 to 105 barInjection Pressure, Low (second stage): 25 to 70 barInjection Velocity: 10 to 80 mm/sec |
| Note Message | |
|---|---|
| 1 . | 150x10x4mm specimen |
| 2 . | 6.70 m/sec |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Marvel™ M50 | SCG Chemicals Co., Ltd. | PE Copolymer | Marvel™ |
| Tecnoflon® FOR 60K | Solvay Specialty Polymers | Fluorelastomer | Tecnoflon® |
| COSMOTHENE® L420 | TPC, The Polyolefin Company (Singapore) Pte Ltd | LDPE | COSMOTHENE® |
| ESTAPROP 1050 V0 HF H | Cossa Polimeri S.r.l. | PP Homopolymer | ESTAPROP |
| Sylvin 8708-84 Grey 9493 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |