Category: | PP, Unspecified , Polypropylene |
Manufacturer: | Mando Advanced Materials Co., Ltd. |
Trademark: | TEKAFIN™ |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | qbtKMZ_TEKAFIN-P730HG.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
P730HG is a unreinforced Compounded-PP. |
General Information | |
---|---|
Uses |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 0.928 | g/cm³ | ASTM D792 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength 1(Break) | 35.3 | MPa | ASTM D638 |
Flexural Modulus 2 | 1720 | MPa | ASTM D790 |
Flexural Strength 3 | 44.1 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (23°C, 3.18 mm) | 29 | J/m | ASTM D256 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Deflection Temperature Under Load (0.45 MPa, Unannealed) | 105 | °C | ASTM D648 |
Flammability | Nominal Value | Test Method | |
---|---|---|---|
Flame Rating | HB | UL 94 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 70.0 to 80.0 | °C | |
Drying Time | 3.0 to 4.0 | hr | |
Rear Temperature | 190 to 210 | °C | |
Middle Temperature | 200 to 230 | °C | |
Front Temperature | 200 to 230 | °C | |
Nozzle Temperature | 210 to 230 | °C | |
Processing (Melt) Temp | 210 to 230 | °C | |
Mold Temperature | 40.0 to 60.0 | °C |
Note Message | |
---|---|
1 . | 50 mm/min |
2 . | 3.0 mm/min |
3 . | 3.0 mm/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
MARPOL® EVA 6055 | Marco Polo International, Inc. | EVA | MARPOL® EVA |
SLOVAMID® 66 GF 25 FRG 5 | Plastcom | Nylon 66 | SLOVAMID® 66 |
Bormed™ LE6609-PH | Borealis AG | LDPE | Bormed™ |
Plenco 04548 (Transfer) | Plastics Engineering Co. | Phenolic | Plenco |
Sylvin 9653-50 Clear 876 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |