Category: | Fluorelastomer , Fluoroelastomer |
Manufacturer: | Greene, Tweed & Co. |
Trademark: | Greene FKM |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | q96IDI_Greene-FKM-761.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Greene FKM 761 is a Fluoroelastomer product. It is available in North America. |
General Information | |
---|---|
Appearance |
|
Forms |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.80 | g/cm³ | ASTM D297 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Rockwell Hardness (M-Scale) | 75 | ASTM D785 | |
Durometer Hardness (Shore A) | 77 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Coefficient of Friction 1 | ASTM D1894 | ||
vs. Itself - Dynamic | 1.1 | ||
vs. Itself - Static | 1.2 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | ASTM D412 | ||
50% Strain | 2.48 | MPa | |
100% Strain | 6.89 | MPa | |
Tensile Strength (Break) | 16.0 | MPa | ASTM D412 |
Tensile Elongation (Break) | 190 | % | ASTM D412 |
Compression Set 2 | ASTM D395 | ||
24°C, 70 hr | 7.0 | % | |
175°C, 166 hr | 24 | % | |
200°C, 22 hr | 12 | % |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Change in Tensile Strength in Air (276°C, 70 hr) | -25 | % | ASTM D573 |
Change in Ultimate Elongation in Air (276°C, 70 hr) | -8.0 | % | ASTM D573 |
Change in Durometer Hardness in Air (Shore A, 276°C, 70 hr) | -1.0 | ASTM D573 | |
Change in Tensile Strength | ASTM D471 | ||
24°C, 70 hr, in Reference Fuel B | -12 | % | |
200°C, 70 hr, in Reference Oil 300 | -12 | % | |
Change in Ultimate Elongation | ASTM D471 | ||
24°C, 70 hr, in Reference Fuel B | 2.0 | % | |
200°C, 70 hr, in Reference Oil 300 | 13 | % | |
Change in Durometer Hardness | ASTM D471 | ||
Shore A, 24°C, 70 hr, in Reference Fuel B | -2.0 | ||
Shore A, 200°C, 70 hr, in Reference Oil 300 | -6.0 | ||
Change in Mass (276°C, 70 hr, in Air) | -8.0 | % | ASTM D471 |
Change in Volume | ASTM D471 | ||
24°C, 70 hr, in Reference Fuel B | 2.3 | % | |
200°C, 70 hr, in Reference Oil 300 | 15 | % |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
CLTE - Flow | 2.2E-4 | cm/cm/°C | ASTM E228 |
Service Temperature | -40 to 232 | °C |
Additional Information | Nominal Value | Test Method | |
---|---|---|---|
Rubber Classification | FKM | ASTM D1418 |
Note Message | |
---|---|
1 . | Method C |
2 . | 25% Deflection |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
MAXAMID™ PA66G33L BK | Pier One Polymers, Inc. | Nylon 66 | MAXAMID™ |
SABIC® Vestolen A RELY 5922R 10000 | Saudi Basic Industries Corporation (SABIC) | HDPE | SABIC® Vestolen A |
XIRAN® IZ1018M | Polyscope Polymers BV | SMA | XIRAN® |
CERTENE™ LDB-222 | Muehlstein | LDPE | CERTENE™ |
Hy-Vin® VR818 | INEOS Compounds | PVC, Rigid | Hy-Vin® |