| Category: | TPU-Polyether , Thermoplastic Polyurethane Elastomer (Polyether) |
| Manufacturer: | BASF Corp. Thermoplastic Polyurethanes |
| Trademark: | Elastollan® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | p8MC9p_Elastollan-1164D.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Elastollan® 1164D exhibits excellent abrasion resistance, toughness, transparency, very good low temperature flexibility, hydrolytic stability and fungus resistance. It has excellent damping characteristics and outstanding resistance to tear propagation. Elastollan® 1164D conforms to the FDA food contact regulations as described in book 21, section 177.2600 for wet food contact applications. Elastollan®1164D also has NSF Standard 61 "Water Contact Material" certification. Elastollan® 1164D is supplied uncolored in diced form. |
| General Information | |
|---|---|
| Features |
|
| Agency Ratings |
|
| Appearance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.18 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore D) | 64 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus (Injection Molded) | 296 | MPa | ASTM D412 |
| Flexural Modulus (Injection Molded) | 255 | MPa | ASTM D790 |
| Taber Abrasion Resistance | 55.0 | mg | ASTM D1044 |
| Abrasion - DIN | 30 | mm³ | DIN 53516 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Softening Point - DMA | 132 | °C | Internal Method |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ASTM D412 | ||
| 100% Strain | 33.1 | MPa | |
| 300% Strain | 44.1 | MPa | |
| Tensile Strength | 49.0 | MPa | ASTM D412 |
| Tensile Elongation (Break) | 390 | % | ASTM D412 |
| Tear Strength 1 | 245 | kN/m | ASTM D624 |
| Compression Set | ASTM D395B | ||
| 23°C, 22 hr | 40 | % | |
| 70°C, 22 hr | 50 | % |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Glass Transition Temperature | 13.0 | °C | Internal Method |
| Vicat Softening Temperature | 128 | °C | ASTM D1525 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 110 to 120 | °C | |
| Drying Time | 2.0 to 3.0 | hr | |
| Suggested Max Moisture | 0.030 | % | |
| Rear Temperature | 210 to 230 | °C | |
| Middle Temperature | 210 to 230 | °C | |
| Front Temperature | 210 to 230 | °C | |
| Nozzle Temperature | 220 to 240 | °C |
| Note Message | |
|---|---|
| 1 . | Die C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Monprene® TL-2563A | Teknor Apex Company | TPE | Monprene® |
| Altuglas® SG7 | Altuglas International of Arkema Inc. | Acrylic (PMMA) | Altuglas® |
| Europrene® 1500 | Versalis S.p.A. | SBR, Emulsion | Europrene® |
| Diakon® Frost 952 70 | Lucite International Inc. | Acrylic (PMMA) | Diakon® |
| Durolon® VR2500 | Unigel Plásticos | PC | Durolon® |