Santoprene™ 8221-85M300

Category: TPV , Thermoplastic Vulcanizate
Manufacturer: ExxonMobil Chemical
Trademark: Santoprene™
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: otdWgm_Santoprene-8221-85M300.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
It is a kind of thermoplastic vulcanized elastomer (TPV) that is hard, colorable and resistant to ultraviolet radiation in the series of thermoplastic elastomers (TPE). This material is suitable for automotive interior applications that require low atomization and good appearance. This brand of Shanduping TPV is a shear rate dependent product that can be processed on conventional thermoplastic injection molding equipment. This is a polyolefin-based material that can be recycled in the production process.
General Information
Features
  • Good UV resistance
  • Recyclable materials
  • Good formability
  • Good coloring
  • High liquidity
  • Ozone resistance
  • Good appearance
Uses
  • Application in Automobile Field
  • Car interior parts
  • Outdoor application
RoHS Compliance
  • RoHS compliance
Appearance
  • Natural color
Forms
  • Particle
Processing Method
  • Multiple injection molding
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity
    -- 0.918g/cm³ASTM D792
    -- 0.920g/cm³ISO 1183
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shaw A, 15 seconds, 23°C, 2.00mm)84ISO 868
ElastomersNominal ValueUnitTest Method
Tensile Stress - Across Flow (100% Strain, 23°C)4.10MPaASTM D412, ISO 37
Tensile Strength - Across Flow (Break, 23°C)9.00MPaASTM D412, ISO 37
Tensile Elongation - Across Flow (Break, 23°C)500%ASTM D412, ISO 37
ThermalNominal ValueUnitTest Method
Brittleness Temperature -59.0°CASTM D746, ISO 812
Additional Information
如果适用,这是基于扇形浇口注塑成型的平板测试结果。拉伸强度、伸长率和拉伸应力沿垂直流动方向测定 - ISO 1 型,ASTM die C。不建议用于热油。从埃克森美孚欧洲分支机构直接购买的所有产品都符合 REACH 法规。 对于埃克森 美孚未进口至欧洲的产品,用户应自行评估其是否满足 REACH 法规。
Legal statement
有关详细的产品监管信息,请联系客户服务。未经埃克森美孚化工书面允许,这种产品包括其产品名称,不得在任何医疗应用领域予以使用或
InjectionNominal ValueUnit
Drying Temperature 82.2°C
Drying Time 3.0hr
Injection instructions
Santoprene TPV与乙缩醛和PVC不相容。更多关于加工和模具设计的信息,请查阅我们的《注射成型指南》。
Resin Grade Manufacturer Category Trademark
Ranger PBT PBT-403-G-M50 Beijing Ranger Chemical Co., Ltd. PBT Ranger PBT
Hifax TRC 277P LyondellBasell Industries PP Copolymer Hifax
Plaslube® PC / PET IM 1016 UV Techmer Engineered Solutions PC+PET Plaslube®
Hostacom X M2 V05 C11354 LyondellBasell Industries PP Copolymer Hostacom
KMI PE LDPE REPRO KMI Group, Inc. LDPE KMI PE