Grilamid® XE 3997 nat is a Polyamide 12 (Nylon 12) material. It is available in Africa & Middle East, Asia Pacific, Europe, Latin America, or North America for blow molding, extrusion, or injection stretch blow molding. Important attributes of Grilamid® XE 3997 nat are:
Typical applications include:
|
General Information | |
---|---|
Features |
|
Uses |
|
Agency Ratings |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.00 | -- | g/cm³ | ISO 1183 |
Molding Shrinkage | ISO 294-4 | |||
Across Flow | 0.80 | -- | % | |
Flow | 0.70 | -- | % | |
Water Absorption | ISO 62 | |||
Saturation, 23°C | 3.0 | -- | % | |
Equilibrium, 23°C, 50% RH | 1.5 | -- | % |
Hardness | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Ball Indentation Hardness | -- | 90.0 | MPa | ISO 2039-1 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus | -- | 1600 | MPa | ISO 527-2 |
Tensile Stress | ISO 527-2 | |||
Yield | -- | 60.0 | MPa | |
Break | -- | 45.0 | MPa | |
Tensile Strain | ISO 527-2 | |||
Yield | -- | 6.0 | % | |
Break | -- | > 50 | % | |
Nominal Tensile Strain at Break | -- | > 50 | % | ISO 527-2 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | |||
-30°C | -- | 12 | kJ/m² | |
23°C | -- | 13 | kJ/m² | |
Charpy Unnotched Impact Strength | ISO 179/1eU | |||
-30°C | -- | No Break | ||
23°C | -- | No Break |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature | ||||
0.45 MPa, Unannealed | 135 | -- | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 115 | -- | °C | ISO 75-2/A |
Continuous Use Temperature | Internal Method | |||
-- 1 | 80.0 to 100 | -- | °C | |
-- 2 | 120 | -- | °C | |
Glass Transition Temperature 3 | 155 | -- | °C | ISO 11357-2 |
CLTE | ISO 11359-2 | |||
Flow | 9.0E-5 | -- | cm/cm/°C | |
Transverse | 9.0E-5 | -- | cm/cm/°C |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Surface Resistivity | -- | 1.0E+12 | ohms | IEC 60093 |
Volume Resistivity | -- | 1.0E+13 | ohms·cm | IEC 60093 |
Electric Strength | -- | 34 | kV/mm | IEC 60243-1 |
Comparative Tracking Index | -- | 600 | V | IEC 60112 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Flammability Classification (0.800 mm) | HB | -- | IEC 60695-11-10, -20 |
Additional Information | Dry | Conditioned | Test Method | |
---|---|---|---|---|
ISO Type | PA MACM12, GT, 14-020 | -- | ISO 1874 |
Note Message | |
---|---|
1 . | Long Term |
2 . | Short Term |
3 . | 10°C/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
SUPREME HIPS SH400M | Supreme Petrochem Ltd. | PS (HIPS) | SUPREME HIPS |
TAIRIREX GP550N | Formosa Plastics Corporation | PS (GPPS) | TAIRIREX |
Adell Polyamide AR-32 | Adell Plastics, Inc. | Nylon 66 | Adell Polyamide |
DIOSHY® GP-965 | DIOSHY Co.,Ltd. | SEBS | DIOSHY® |
LNP™ LUBRICOMP™ RP004 compound | SABIC Innovative Plastics | Nylon 66 | LNP™ LUBRICOMP™ |