| Category: | Nylon 66 , Polyamide 66 |
| Manufacturer: | Ravago Manufacturing Americas, LLC |
| Trademark: | Hylon® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | onLGgg_Hylon-N1243HL.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Nylon 66, 43% Glass Filled |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| RoHS Compliance |
|
| UL File Number |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.49 | g/cm³ | ISO 1183 |
| Molding Shrinkage - Flow (3.18 mm) | 0.30 to 0.50 | % | ISO 294-4 |
| Water Absorption (23°C, 24 hr) | 0.60 | % | ISO 62 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Rockwell Hardness (M-Scale) | 103 | ISO 2039-2 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Break) | 183 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 2.0 | % | ISO 527-2 |
| Flexural Modulus | 9650 | MPa | ISO 178 |
| Flexural Stress | 248 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength | 9.0 | kJ/m² | ISO 180 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 252 | °C | ISO 75-2/A |
| Flammability | Nominal Value | Test Method | |
|---|---|---|---|
| Flame Rating (1.50 mm) | HB | UL 94 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| XYRON™ 1951J | Asahi Kasei Chemicals Corporation | PPE+PS | XYRON™ |
| Hostaform® C 27021 LS colored | Celanese Corporation | Acetal (POM) Copolymer | Hostaform® |
| MAJORIS DG308X - 8229 | AD majoris | PP, Unspecified | MAJORIS |
| Sylvin 6416-70 Blue 8438 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
| Tunhe PET TH103 | Xinjiang Blueridge Tunhe Chemical Industry Co.,Ltd | PET | Tunhe PET |