| Category: | TPO (POE) , Thermoplastic Polyolefin Elastomer |
| Manufacturer: | Multibase, A Dow Corning Company |
| Trademark: | Multi-Flex® TPO |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | ogfauU_Multi-Flex-TPO-1047-S.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Multi-Flex® TPO 1047 S is a Thermoplastic Polyolefin Elastomer (TPO (POE)) product. It is available in Europe or North America. Typical application: Automotive. Characteristics include:
|
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 0.908 | g/cm³ | ASTM D792 |
| Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 3.6 | g/10 min | ASTM D1238 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore D, 10 sec) | 46 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flexural Modulus | 352 | MPa | ASTM D790 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength (Break) | 13.1 | MPa | ASTM D412 |
| Tensile Elongation (Break) | 600 | % | ASTM D412 |
| Tear Strength | 99.8 | kN/m | ASTM D624 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 65.6 | °C | |
| Drying Time | 2.0 to 4.0 | hr | |
| Rear Temperature | 199 | °C | |
| Middle Temperature | 210 | °C | |
| Front Temperature | 166 | °C | |
| Nozzle Temperature | 227 | °C | |
| Processing (Melt) Temp | 227 | °C | |
| Mold Temperature | 32.2 to 48.9 | °C | |
| Injection Rate | Fast |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| NOVAPOL® TF-Y822 Series | NOVA Chemicals | LLDPE | NOVAPOL® |
| ENGAGE™ 7387 EL | The Dow Chemical Company | TPO (POE) | ENGAGE™ |
| Hipolyene 8110 | Zylog Plastalloys | TPO (POE) | Hipolyene |
| Larton G/40 I6 | LATI S.p.A. | PPS | Larton |
| LUVOCOM® 19/CF/30 | LEHVOSS Group | Nylon 46 | LUVOCOM® |