| Category: | Nylon 66 , Polyamide 66 |
| Manufacturer: | EMAS Plastik San.Tic.AS. |
| Trademark: | EMLON® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | oNe1yw_EMLON-66-MTF-20-FR-V2.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Polyamide 66, %25 talcum filled, V2 flammability |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Recycled Content |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.25 to 1.28 | g/cm³ | ISO 1183 |
| Molding Shrinkage | 0.70 to 0.90 | % |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Shore Hardness (Shore D) | 75 to 85 | ISO 868 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 4000 to 6000 | MPa | ISO 527-2 |
| Tensile Stress (Yield) | 120 to 140 | MPa | ISO 527-2 |
| Tensile Strain (Break) | > 3.0 | % | ISO 527-2 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength | > 15 | kJ/m² | ISO 180/1A |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 250 | °C | ISO 75-2/A |
| Vicat Softening Temperature | 250 | °C | ISO 306/B |
| Melting Temperature (DSC) | 265 | °C | ISO 3146 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flame Rating | V-2 | UL 94 | |
| Glow Wire Ignition Temperature | 750 | °C | VDE 0471/2 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| WPP PP PPC4TF1.3-Natural | Washington Penn Plastic Co. Inc. | PP Copolymer | WPP PP |
| UBE Nylon 1024JI | UBE Engineering Plastics, S.A. | Nylon 6 | UBE Nylon |
| UNIPA® MLo | Nytef Plastics, Ltd. | Nylon 6 | UNIPA® |
| ENGAGE™ HM 7289 | The Dow Chemical Company | TPO (POE) | ENGAGE™ |
| OpteSTAT™ NC TPU 9020 | Ovation Polymers Inc. | TPU, Unspecified | OpteSTAT™ |