| Category: | PUR-Ether/TDI , Polyurethane (Polyether, TDI) |
| Manufacturer: | Anderson Development Company |
| Trademark: | Andur |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | oIypVT_Andur-7003-AP-F-Curene-89-LC.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Andur 7003AP-F is a polyether (PPG) based liquid, toluene diisocyanate terminated prepolymer. A water-white clear elastomer with a hardness of 70 Shore A is obtained when this prepolymer is cured with Curene 89-LC. Elastomers of lower hardness can be obtained through the use of plasticizers. |
| General Information | |
|---|---|
| Forms |
|
| Hardness | Nominal Value | Test Method | |
|---|---|---|---|
| Durometer Hardness (Shore A) | 70 | ASTM D2240 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ASTM D412 | ||
| 100% strain | 3.17 | MPa | ASTM D412 |
| 300% strain | 4.83 | MPa | ASTM D412 |
| Tensile Strength (Yield) | 22.8 | MPa | ASTM D412 |
| Tensile Elongation (Break) | 730 | % | ASTM D412 |
| Bayshore Resilience | 73 | % | ASTM D2632 |
| Thermoset | Nominal Value | Unit | |
|---|---|---|---|
| Pot Life | 0.75 - 1.0 | min | |
| Demold Time (100°C) | 8.0 | min |
| Additional Information |
|---|
| Durometer Hardness, ASTM D2240, Shore A: 69 to 71Die C Tear, ASTM D1004: 220 pliAverage Split Tear, ASTM D1938: 92 pliStoichiometry Curative Level: 97%Mix Temperature: Andur 7003 AP-F: 110-160°F Curene 89-LC: 72°F |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Mold Temperature | 22.2 - 100 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 207A TFE 13 SI 2 HS | RTP Company | Nylon 6 | RTP |
| T & T Marketing TD 150 FR Natural | T & T Marketing, Inc. | TP, Unspecified | T & T Marketing |
| TRAMID® 4115 | Samyang Corporation | Nylon, Unspecified | TRAMID® |
| Nipol® N917 | Zeon Chemicals L.P. | NBR | Nipol® |
| Alcryn® 2165 TR | Advanced Polymer Alloys | MPR | Alcryn® |