| Category: | TPE , Thermoplastic Elastomer |
| Manufacturer: | API SpA |
| Trademark: | apinat® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | oIyaiA_apinat-A-70.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
apinat®A 70 is a thermoplastic elastomer (TPE) product,. It can be processed by extrusion or injection molding and is available in Europe. Typical application areas are: engineering/industrial accessories. Features include:
|
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Agency Ratings |
|
| Appearance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.19 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A, 15 sec) | 71 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength | ASTM D638 | ||
| -- | 10.0 | MPa | ASTM D638 |
| 100% strain | 2.50 | MPa | ASTM D638 |
| 300% strain | 5.00 | MPa | ASTM D638 |
| Tensile Elongation (Break) | 750 | % | ASTM D638 |
| Abrasion Resistance | 150 | mm³ | DIN 53516 |
| Additional Information | Nominal Value | ||
|---|---|---|---|
| Ozone Resistance 1(40°C) | Good |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tear Strength | 45.0 | kN/m | ASTM D624 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 80.0 | °C | |
| Drying Time | 2.0 | hr | |
| Suggested Max Moisture | 0.10 | % | |
| Rear Temperature | 120 - 140 | °C | |
| Middle Temperature | 130 - 150 | °C | |
| Front Temperature | 140 - 160 | °C | |
| Nozzle Temperature | 150 - 170 | °C | |
| Mold Temperature | 25.0 - 35.0 | °C | |
| Injection Rate | Moderate-Fast |
| Injection instructions |
|---|
| Injection Pressure: MediumBack Pressure: Low to Medium |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 80.0 | °C | |
| Drying Time | 2.0 | hr | |
| Suggested Max Moisture | 0.10 | % | |
| Cylinder Zone 1 Temp. | 110 - 130 | °C | |
| Cylinder Zone 2 Temp. | 130 - 140 | °C | |
| Cylinder Zone 3 Temp. | 135 - 145 | °C | |
| Cylinder Zone 4 Temp. | 140 - 150 | °C | |
| Die Temperature | 140 - 150 | °C |
| Extrusion instructions |
|---|
| L/D Ratio: >20Compression Ratio: 1:2.5 |
| Note Message | |
|---|---|
| 1 . | 72 hr, 200 ppcm, Tension = 20% |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Sinelec CCB6965 | Teknor Apex Asia Pacific PTE. LTD. | PS (Specialty) | Sinelec |
| Boda BDF-KK2802 | Chenguang Fluoro & Silicone Elastomers Co., Ltd. | Fluorelastomer | Boda |
| HiPrene® MT52VF | GS Caltex | PP, Unspecified | HiPrene® |
| Innothane® FM-110 | Innovative Polymers, Inc. | TSU | Innothane® |
| KEBAFORM® C 902 FA | BARLOG plastics GmbH | Acetal (POM) Copolymer | KEBAFORM® C |