| Category: | Nylon 66 , Polyamide 66 |
| Manufacturer: | Kunststoff-Kontor-Hamburg GmbH |
| Trademark: | GERMAMID |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | nxISVn_GERMAMID-6-6-HSZ.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| GERMAMID 6.6 HSZ is a polyamide 66 (nylon 66) material,. This product is available in Europe,. The main characteristics of GERMAMID 6.6 HSZ are impact modification. |
| General Information | |
|---|---|
| Additive |
|
| Features |
|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.08 | g/cm³ | ISO 1183 |
| Molding Shrinkage | 1.2 - 2.5 | % | ISO 294-4 |
| Water Absorption (Saturation, 23°C) | 2.1 | % | ISO 62 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 2200 | MPa | ISO 527-2 |
| Tensile Stress (Yield) | 50.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 50 | % | ISO 527-2 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | No Break | ISO 179/1eA | |
| Charpy Unnotched Impact Strength | No Break | ISO 179/1eU |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (0.45 MPa, Unannealed) | 75.0 | °C | ISO 75-2/B |
| Melting Temperature | 255 | °C | |
| Thermal Conductivity | 0.23 | W/m/K | ISO 8302 |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Surface Resistivity | 1.0E+12 | ohms | IEC 60093 |
| Additional Information |
|---|
| Tensile Strain at Break, ISO 527: >50% |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 2581.3 | RTP Company | PC+ABS | RTP |
| Talcoprene® 1020TCD NAT | SO.F.TER. SPA | PP Homopolymer | Talcoprene® |
| Veroplas T150 | PlastxWorld Inc. | ABS | Veroplas |
| Generic PBT - Aramid Fiber | Generic | PBT | Generic |
| Epolene® C-23 | Westlake Chemical Corporation | LDPE | Epolene® |