apilon 52® ETC 42

Category: TPU-Polyether , Thermoplastic Polyurethane Elastomer (Polyether)
Manufacturer: API SpA
Trademark: apilon 52®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: ntlNNN_apilon-52-ETC-42.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
apilon 52®ETC 42 is a thermoplastic polyurethane elastomer (polyether)(TPU-polyether) product,. It can be processed by extrusion or injection molding and is available in Europe. apilon 52®The application areas of ETC 42 include engineering/industrial accessories, electrical/electronic applications, electrical appliances, tools and home applications.

Features include:
  • chemical resistance
  • environmental protection/green
  • low temperature resistance
  • Wear-resistant
General Information
Features
  • Antimicrobial
  • Recyclable materials
  • Good wear resistance
  • Low temperature resistance
  • Good chemical resistance
  • Hydrolysis resistance
  • Oil resistance
Uses
  • Handle
  • Wheels
  • Conveyor belt repair
  • Electrical/Electronic Applications
  • Electrical appliances
  • Washer
  • Power/other tools
  • Pipe fittings
  • Household goods
  • Sporting goods
  • Coating application
  • Footwear
Forms
  • Particle
Processing Method
  • Extrusion
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.13g/cm³ASTM D792
HardnessNominal ValueUnitTest Method
Durometer Hardness ASTM D2240
    Shaw A, 15 seconds 87ASTM D2240
    Shaw D, 3 seconds 37ASTM D2240
MechanicalNominal ValueUnitTest Method
Tensile Strength ASTM D638
    -- 38.5MPaASTM D638
    100% strain 6.00MPaASTM D638
    300% strain 9.70MPaASTM D638
Tensile Elongation (Break)640%ASTM D638
Abrasion Resistance 50.0mm³DIN 53516
ElastomersNominal ValueUnitTest Method
Tear Strength 193.0kN/mASTM D624
ImpactNominal ValueUnitTest Method
Notched Izod Impact (-20°C)No BreakASTM D256
InjectionNominal ValueUnit
Drying Temperature 80.0 - 110°C
Drying Time 2.0hr
Suggested Max Moisture 0.070%
Rear Temperature 180 - 190°C
Middle Temperature 185 - 200°C
Front Temperature 190 - 215°C
Nozzle Temperature 200 - 230°C
Mold Temperature 30.0 - 60.0°C
Injection Pressure 50.0 - 100MPa
Injection Rate Slow-Moderate
Injection instructions
Back Pressure: Medium to LowLocking Pressure: High
ExtrusionNominal ValueUnit
Drying Temperature 80.0 - 110°C
Drying Time 2.0hr
Suggested Max Moisture 0.070%
Cylinder Zone 1 Temp. 160 - 185°C
Cylinder Zone 2 Temp. 170 - 200°C
Cylinder Zone 3 Temp. 175 - 210°C
Cylinder Zone 4 Temp. 180 - 220°C
Die Temperature 170 - 210°C
Extrusion instructions
L/D Ratio: 20:1 to 30:1Compression Ratio: 1:2.5 to 1:3
Note Message
1 .Without Notch
Resin Grade Manufacturer Category Trademark
Sasol Polymers PE LT033 (Film Extrusion) Sasol Polymers LDPE Sasol Polymers PE
Shandong Nylon A4TR02 Shandong Dongchen Engineering Plastics Co., Ltd. Nylon, Unspecified Shandong Nylon
Durethan® BM 25 FN20 DUS013 000000 LANXESS GmbH Nylon 6 Durethan®
Karina GRAY PVC COMPOUND 70900-18/229-H-IS Karina Ind. e Com. de Plásticos Ltda PVC, Unspecified Karina
LNP™ LUBRICOMP™ RL003 compound SABIC Innovative Plastics Nylon 66 LNP™ LUBRICOMP™