Category: | Nylon 66 , Polyamide 66 |
Manufacturer: | Next Polymers Ltd. |
Trademark: | Next Nylon 66 Prime Series |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | naUCmR_Next-Nylon-66-Prime-Series-PXF-01NC.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Description PA66 Un Filled FR Natural Compound Product Applications Typical Application includes Terminal box, Electrical cooling fan, and housing Fuse Box, and carriers etc Benefits Good heat aging characteristics RTI (Mechanical) listing up to 140 *C, Halogen and Red phosphorous Free, Execellent CTI Value, Easy processing, V0 Listing at 0.4mm |
General Information | |
---|---|
Features |
|
Uses |
|
Agency Ratings |
|
RoHS Compliance |
|
Appearance |
|
Processing Method |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Specific Gravity | 1.18 | -- | g/cm³ | ASTM D792 |
Molding Shrinkage | ASTM D955 | |||
Flow | 1.1 | -- | % | |
Across Flow | 1.1 | -- | % | |
Water Absorption | ASTM D570 | |||
23°C, 24 hr | 1.5 | -- | % | |
Saturation 1 | 7.5 | -- | % |
Hardness | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Rockwell Hardness (R-Scale) | 120 | -- | ASTM D785 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus | 3600 | 2100 | MPa | ASTM D638 |
Tensile Strength | 80.0 | 55.0 | MPa | ASTM D638 |
Tensile Elongation (Break) | 6.0 | 15 | % | ASTM D638 |
Flexural Modulus | 3200 | 1900 | MPa | ASTM D790 |
Flexural Strength | 110 | 80.0 | MPa | ASTM D790 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength (23°C) | 6.00 | 9.00 | kJ/m² | ASTM D256 |
Notched Izod Impact (23°C) | 49 | 78 | J/m | ASTM D256 |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Deflection Temperature Under Load | ASTM D648 | |||
0.45 MPa, Unannealed | 225 | -- | °C | |
1.8 MPa, Unannealed | 85.0 | -- | °C | |
Melting Temperature | 260 | -- | °C | ASTM D2117 |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Surface Resistivity | 1.0E+15 | -- | ohms | IEC 60093 |
Volume Resistivity | 1.0E+15 | -- | ohms·cm | IEC 60093 |
Electric Strength | 18 | -- | kV/mm | IEC 60243-1 |
Comparative Tracking Index | 600 | -- | V | IEC 60112 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Flame Rating (0.800 mm) | V-0 | -- | UL 94 | |
Glow Wire Flammability Index (0.800 mm) | 960 | -- | °C | IEC 60695-2-12 |
Oxygen Index | 28 | -- | % | ASTM D2863 |
Injection | Dry | Unit | |
---|---|---|---|
Drying Temperature - Hot Air Dryer | 80.0 | °C | |
Drying Time | 4.0 to 6.0 | hr | |
Suggested Max Moisture | 0.20 | % | |
Rear Temperature | 260 to 265 | °C | |
Middle Temperature | 265 to 270 | °C | |
Front Temperature | 265 to 270 | °C | |
Mold Temperature | 65.0 to 85.0 | °C |
Note Message | |
---|---|
1 . | Immersed |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Polylink Polymer P-51030-GF(N) | Polylink Polymers (India) Ltd. | Nylon 6 | Polylink Polymer |
RTP 2103-6 | RTP Company | PEI | RTP |
STYRON A-TECH™ 1115 | Americas Styrenics LLC | PS (HIPS) | STYRON A-TECH™ |
Tufel® II 94305 | Momentive Performance Materials Inc. | Silicone | Tufel® II |
Kemcor HD 2990 | Qenos Pty Ltd | HDPE | Kemcor |