| Category: | TPV , Thermoplastic Vulcanizate |
| Manufacturer: | Elastron USA, Inc. |
| Trademark: | Elastron® V |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | nZDHrf_Elastron-V-V201-A90-N.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
A soft, colorable thermoplastic vulcanizate, TPV (EPDM/PP) in the thermoplastic elastomer (TPE) family that offers higher temperature resistance and excellent compression set with superior UV resistance. Bondable to: PP, EVA, PE |
| General Information | |
|---|---|
| Features |
|
| RoHS Compliance |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 0.960 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A) | 90 | ASTM D2240 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ASTM D412 | ||
| 100% Strain | 6.10 | MPa | |
| 300% Strain | 7.60 | MPa | |
| Tensile Strength (Break) | 13.8 | MPa | ASTM D412 |
| Tensile Elongation (Break) | 600 | % | ASTM D412 |
| Tear Strength | 76.0 | kN/m | ASTM D624 |
| Compression Set | ASTM D395 | ||
| 23°C, 22 hr | 35 | % | |
| 70°C, 22 hr | 49 | % | |
| 100°C, 22 hr | 55 | % |
| Additional Information | Nominal Value | Test Method | |
|---|---|---|---|
| Ozone Resistance - Stressed | No Cracks | ASTM D518 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 90.0 | °C | |
| Drying Time | 2.0 | hr | |
| Suggested Max Regrind | 20 | % | |
| Rear Temperature | 155 to 175 | °C | |
| Middle Temperature | 165 to 185 | °C | |
| Front Temperature | 175 to 195 | °C | |
| Nozzle Temperature | 195 to 225 | °C | |
| Mold Temperature | 25.0 to 50.0 | °C |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 90.0 | °C | |
| Drying Time | 2.0 | hr | |
| Cylinder Zone 1 Temp. | 160 to 180 | °C | |
| Cylinder Zone 2 Temp. | 165 to 185 | °C | |
| Cylinder Zone 3 Temp. | 170 to 190 | °C | |
| Cylinder Zone 4 Temp. | 185 to 205 | °C | |
| Cylinder Zone 5 Temp. | 190 to 220 | °C | |
| Die Temperature | 195 to 225 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Westlake LLDPE LF2010 | Westlake Chemical Corporation | LLDPE | Westlake LLDPE |
| ACRYPET® MD | Mitsubishi Rayon Co., Ltd. | Acrylic (PMMA) | ACRYPET® |
| Bergamid™ B70 W25 | PolyOne Corporation | Nylon 6 | Bergamid™ |
| API PS 410 | American Polymers, Inc. | PS (GPPS) | API PS |
| Hytrel® 30HS | DuPont Performance Polymers | TPC-ET | Hytrel® |