Category: | TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester) |
Manufacturer: | Huntsman Corporation |
Trademark: | AVALON® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | nQQHma_AVALON-75-ABX.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
AVALON 75 ABX is a high performance polyester based thermoplastic polyurethane for injection moulding. AVALON 75 ABX is part of the AVALON Perform Range and offers a specially designed, flexible material with improved slip resistance and rubber-like properties, particularly suitable for TPU/PU applications. The features offered include:
|
General Information | |
---|---|
Features |
|
Uses |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.14 | g/cm³ | DIN 53479 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A) | 75 | DIN 53505 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Abrasion Resistance | mm³ | DIN 53516 | |
Bending life | > 1.0E+5 | Cycles | DIN 53522 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (Break) | > 25.0 | MPa | DIN 53504 |
Tensile Elongation (Break) | > 750 | % | DIN 53504 |
Tear Strength 1 | > 35 | kN/m | DIN 53507 |
Additional Information |
---|
Test plates conditioned 20 hours at 100°C before testing |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature - Desiccant Dryer | 80.0 - 90.0 | °C | |
Drying Time - Desiccant Dryer | 2.0 | hr | |
Hopper Temperature | 25.0 - 35.0 | °C | |
Rear Temperature | 160 - 180 | °C | |
Middle Temperature | 165 - 185 | °C | |
Front Temperature | 165 - 190 | °C | |
Nozzle Temperature | 160 - 185 | °C | |
Mold Temperature | 25.0 - 50.0 | °C | |
Injection Pressure | 2.00 - 10.0 | MPa | |
Injection Rate | Slow | ||
Holding Pressure | 1.00 - 5.00 | MPa | |
Back Pressure | 0.0300 - 0.300 | MPa | |
Screw Speed | 20 - 80 | rpm | |
Screw L/D Ratio | 20.0:1.0 to 25.0:1.0 | ||
Screw Compression Ratio | 2.0 : 1.0 - 3.0 : 1.0 |
Injection instructions |
---|
Typical Screw Diameter : 40 - 120 mm3 Stage Design Feed Zone : 0.4L Compression Zone : 0.3L Metering Zone : 0.3L |
Note Message | |
---|---|
1 . | Method B, right-angle specimen (without cut) |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Polylink Power Cable PP 409/401 (S) | Polylink Polymers (India) Ltd. | XLPE | Polylink Power Cable |
Nanjing Hongrui PP P860 | Nanjing Hongrui Engineering Plastics Co., Ltd. | PP, Unspecified | Nanjing Hongrui PP |
Anjacom® R500 | Almaak International GmbH | ABS | Anjacom® |
Aquamix™ 568 | PolyOne Corporation | Latex | Aquamix™ |
Karina ORANGE COLOR CONCENTRATE 32/19-G | Karina Ind. e Com. de Plásticos Ltda | PVC, Unspecified | Karina |