| Category: | Nylon 6 , Polyamide 6 |
| Manufacturer: | DOMO Engineering Plastics SPA |
| Trademark: | DOMAMID® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | nAm7fW_DOMAMID-6G30HCE.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Polyamide 6, 30% glass fibre, for injection moulding. |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.36 | g/cm³ | ISO 1183 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 10000 | MPa | ISO 527-2/1 |
| Tensile Stress (Break) | 180 | MPa | ISO 527-2/5 |
| Tensile Strain (Break) | 3.5 | % | ISO 527-2/5 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength (23°C) | 14 | kJ/m² | ISO 180/1A |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Melting Temperature | 218 to 222 | °C | ISO 11357-3 |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Surface Resistivity | 1.0E+13 | ohms | IEC 60093 |
| Volume Resistivity | 1.0E+15 | ohms·cm | IEC 60093 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Burning Rate | < 100 | mm/min | FMVSS 302 |
| Flame Rating (0.800 mm) | HB | UL 94 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 75.0 to 95.0 | °C | |
| Drying Time | 4.0 to 6.0 | hr | |
| Processing (Melt) Temp | 240 to 270 | °C | |
| Mold Temperature | 90.0 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| MTEGRITY™ LLDPE LL104MM | M. Holland Company | LLDPE | MTEGRITY™ LLDPE |
| Baydur® GS-772 | Covestro - PUR | PUR-MDI | Baydur® |
| CALP 4359G | Lion Idemitsu Composites Co., Ltd. | Polyolefin, Unspecified | CALP |
| LUVOCOM® 1114-8364 | Lehmann & Voss & Co. | PAEK | LUVOCOM® |
| Kinta R4-006 Colored | Kinta Technology (Hong Kong) Co., Ltd. | PPS | Kinta |