| Category: | SBR, Emulsion , Emulsion Styrene Butadiene Rubber |
| Manufacturer: | SIBUR |
| Trademark: | SIBUR Synthetic Rubber |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | n658c5_SIBURSyntheticRubberSBR1502.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Synthetic rubber SBR-1502 is is obtained by copolymerization of butadiene with a-methylstyrene at a temperature of (4-8)°C where used as emulsifier is a mixture of disproportionated rosin and synthetic fatty acid soaps or complex emulsifiers. Medium Mooney viscosity. Product characteristics: Appearance - bale of light-yellow to brown color; weight of a bale - (30 ± 1) kg; packing - a plastic container; shelf life - one (1) year since the date of manufacture |
| General Information | |
|---|---|
| Additive |
|
| Features |
|
| Appearance |
|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Mooney Viscosity (ML 1+4, 100°C) | 45 - 57 | MU | ASTM D1646 |
| Bound Styrene | 21.0 - 24.0 | % | Internal method |
| Organic Acid | 5.0 - 7.2 | % | ASTM D5774 |
| Soap - Organic Acid | % | ASTM D5774 | |
| Ash Content | % | ASTM D5667 | |
| Volatile Matter | % | ASTM D5668 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (300% Strain) | > 9.80 | MPa | ASTM D3185 |
| Tensile Strength (Yield) | > 22.0 | MPa | ASTM D3185 |
| Tensile Elongation (Break) | 400 - 650 | % | ASTM D3185 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Sarlink® TPV 2555 | Teknor Apex Company | TPV | Sarlink® TPV |
| Axiall PVC 1802 Clear 7070 | Axiall Corporation | PVC, Flexible | Axiall PVC |
| Flontech® FT-M01-1 | Guarniflon S.p.A. - Flontech Division | PTFE | Flontech® |
| elitel UE3690 | UNITIKA Plastics Division | TPC-ET | elitel |
| Iupilon® MB8500 | Mitsubishi Engineering-Plastics Corp | PC+ABS | Iupilon® |