Category: | Nylon 6 , Polyamide 6 |
Manufacturer: | A. Schulman Europe |
Trademark: | SCHULAMID® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | mrbidi_SCHULAMID-6-GF-30-HI-FR-4.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
30% glass fibre reinforced and impact modified PA 6; flame retardant containing halogens without PBDE |
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Processing Method |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.59 | -- | g/cm³ | ISO 1183/A |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus | 11000 | 8500 | MPa | ISO 527-2/1A/1 |
Tensile Stress (Break) | 150 | 104 | MPa | ISO 527-2/1A/5 |
Tensile Strain (Break) | 2.5 | 4.0 | % | ISO 527-2/1A/5 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | |||
-30°C | 8.5 | -- | kJ/m² | |
23°C | 10 | 12 | kJ/m² | |
Charpy Unnotched Impact Strength | ISO 179/1eU | |||
-30°C | 54 | -- | kJ/m² | |
23°C | 60 | 65 | kJ/m² |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature | ||||
0.45 MPa, Unannealed | 216 | -- | °C | ISO 75-2/Bf |
1.8 MPa, Unannealed | 207 | -- | °C | ISO 75-2/Af |
Vicat Softening Temperature | ||||
-- | 211 | -- | °C | ISO 306/A120 |
-- | 203 | -- | °C | ISO 306/B50 |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Surface Resistivity | > 1.0E+15 | -- | ohms | IEC 60093 |
Volume Resistivity | > 1.0E+13 | -- | ohms·cm | IEC 60093 |
Comparative Tracking Index | 225 | -- | V | IEC 60112 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Flammability Classification | IEC 60695-11-10, -20 | |||
0.800 mm | V-0 | -- | ||
1.60 mm | V-2 | -- | ||
Glow Wire Flammability Index | IEC 60695-2-12 | |||
0.750 mm | 960 | -- | °C | |
1.50 mm | 960 | -- | °C | |
3.00 mm | 960 | -- | °C | |
Glow Wire Ignition Temperature | IEC 60695-2-13 | |||
0.750 mm | 800 | -- | °C | |
1.50 mm | 800 | -- | °C | |
3.00 mm | 800 | -- | °C | |
Oxygen Index | 34 | -- | % | ISO 4589-2 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
TES J-1200/30 | Techmer Engineered Solutions | ABS | TES |
Zhongfa PP ZF-T20 | Yuyao Zhongfa Engineering Plastics Co. Ltd. | PP, Unspecified | Zhongfa |
ANSABLEND A15 000 0000 T65 V0 | Daloga srl | PC+ABS | ANSABLEND |
Elastron® V P.V101.A55.B | Elastron USA, Inc. | TPV | Elastron® V |
Karina CLEAR PVC COPOUND -E 65/207-IS | Karina Ind. e Com. de Plásticos Ltda | PVC, Unspecified | Karina |