| Category: | Nylon 66 , Polyamide 66 |
| Manufacturer: | Wellman Engineering Resins |
| Trademark: | Wellamid® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | mhlkkY_Wellamid-22LH-N.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Wellamid® 22LH-N is a Polyamide 66 (Nylon 66) material. It is available in Asia Pacific, Europe, Latin America, or North America for injection molding. Primary attribute of Wellamid® 22LH-N: Flame Rated. Typical application of Wellamid® 22LH-N: Automotive |
| General Information | |
|---|---|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.14 | g/cm³ | ISO 1183 |
| Molding Shrinkage | ISO 294-4 | ||
| Across Flow : 23°C | 2.1 to 2.5 | % | |
| Flow | 2.0 to 2.4 | % |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Yield, 23°C) | 85.0 | MPa | ISO 527-2 |
| Tensile Strain (Yield, 23°C) | 40 | % | ISO 527-2 |
| Flexural Modulus (23°C) | 2900 | MPa | ISO 178 |
| Flexural Stress (23°C) | 105 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength (23°C) | 5.5 | kJ/m² | ISO 180 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 70.0 | °C | ISO 75-2/A |
| Melting Temperature (DSC) | 260 | °C | ISO 3146 |
| Flammability | Nominal Value | Test Method | |
|---|---|---|---|
| Flame Rating (0.750 mm) | V-2 | UL 94 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 79.4 | °C | |
| Drying Time | 2.0 to 4.0 | hr | |
| Suggested Max Moisture | 0.20 | % | |
| Rear Temperature | 277 to 293 | °C | |
| Middle Temperature | 271 to 288 | °C | |
| Front Temperature | 266 to 282 | °C | |
| Nozzle Temperature | 266 to 293 | °C | |
| Processing (Melt) Temp | 271 to 304 | °C | |
| Mold Temperature | 71.1 to 93.3 | °C | |
| Injection Pressure | 34.5 to 138 | MPa | |
| Back Pressure | 0.345 | MPa | |
| Screw Speed | 30 to 120 | rpm |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| ResinDirect HOPP35 | ResinDirect | PP Homopolymer | ResinDirect |
| SCHULADUR® A1 GF 30 LW | A. Schulman Europe | PBT+PET | SCHULADUR® |
| Hipolyene 8021 M | Zylog Plastalloys | TPO (POE) | Hipolyene |
| Huaxia Shenzhou PFA DS708-A | Shandong Huaxia Shenzhou New Material Co., Ltd. | PFA | Huaxia Shenzhou |
| PLANAC BT-2215 | TOYOBO America, Inc. | PBT | PLANAC |