| Category: | PP, Unspecified , Polypropylene |
| Manufacturer: | Polykemi AB |
| Trademark: | POLYfill |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | mO6fHx_POLYfill-PP-TOUCH-34725.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Glass fibre-reinforced |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.07 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 3.0 | g/10 min | ISO 1133 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore D, 15 sec) | 47 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flexural Modulus (23°C) | 1600 | MPa | ISO 178 |
| Flexural Stress | 32.0 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179 | ||
| -30°C | 10 | kJ/m² | |
| 23°C | 20 | kJ/m² |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature 1(0.45 MPa, Unannealed) | 99.0 | °C | ISO 75-2/B |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flame Rating (1.60 mm) | HB | UL 94 | |
| Glow Wire Ignition Temperature (2.00 mm) | 750 | °C | IEC 60695-2-13 |
| Note Message | |
|---|---|
| 1 . | 120°C/hr |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 200 AR 10 TFE 15 | RTP Company | Nylon 66 | RTP |
| TPSiV™ 3345-65A NAT 25564 | Multibase, A Dow Corning Company | TPSiV | TPSiV™ |
| ECP 2809 | TBA Electro Conductive Products Ltd. | Acrylic, Unspecified | ECP |
| Elastron® V V101.A79.B | Elastron USA, Inc. | TPV | Elastron® V |
| Sylvin 8200-77 Clear 876 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |