| Category: | Nylon 66 , Polyamide 66 |
| Manufacturer: | Teknor Apex Asia Pacific PTE. LTD. |
| Trademark: | Chemlon S |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | m5kHlH_Chemlon-S-125-GVH.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Chemlon S 125 GVH is a Polyamide 66 (Nylon 66) material filled with 25% glass fiber. It is available in Asia Pacific, Europe, or North America for injection molding. Primary attribute of Chemlon S 125 GVH: Flame Rated. Typical applications include:
|
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Features |
|
| Uses |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.55 | g/cm³ | ASTM D792 |
| Molding Shrinkage - Flow | 0.10 to 0.30 | % | ASTM D955 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength (Ultimate) | 135 | MPa | ASTM D638 |
| Tensile Elongation | ASTM D638 | ||
| Yield | 2.0 | % | |
| Break | 2.5 | % | |
| Flexural Modulus | 6850 | MPa | ASTM D790 |
| Flexural Strength | 175 | MPa | ASTM D790 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact (23°C) | 85 | J/m | ASTM D256 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Deflection Temperature Under Load (1.8 MPa, Annealed) | 235 | °C | ASTM D648 |
| Melting Temperature | 257 | °C | ASTM D789 |
| CLTE - Flow | 5.5E-5 | cm/cm/°C | ASTM D696 |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Volume Resistivity | 1.0E+15 | ohms·cm | IEC 60093 |
| Dielectric Strength | 16 | kV/mm | ASTM D149 |
| Comparative Tracking Index (CTI) | 350 | V | UL 746 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flame Rating (0.800 mm) | V-0 | UL 94 | |
| Glow Wire Flammability Index (3.20 mm) | 960 | °C | IEC 60695-2-12 |
| Glow Wire Ignition Temperature (3.20 mm) | 875 | °C | IEC 60695-2-13 |
| Oxygen Index | 32 | % | ASTM D2863 |
| FMVSS Flammability | PASSED |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 80.0 | °C | |
| Suggested Max Moisture | 0.20 | % | |
| Rear Temperature | 252 to 268 | °C | |
| Middle Temperature | 263 to 285 | °C | |
| Front Temperature | 268 to 291 | °C | |
| Nozzle Temperature | 268 to 285 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Melos™ FM 1239 | Melos GmbH | TPO (POE) | Melos™ |
| Milastomer™ 5020NS | Mitsui Chemicals America, Inc. | TPV | Milastomer™ |
| Fireguard® 910L16-C1A-NL1 | Teknor Apex Company | PVC, Flexible | Fireguard® |
| Polifil® Nylon 627 | The Plastics Group | Nylon 66 | Polifil® Nylon |
| Sylvin 5132-75 Clear | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |