| Category: | EVA , Ethylene Vinyl Acetate Copolymer Resin |
| Manufacturer: | ExxonMobil Chemical |
| Trademark: | Escorene™ Ultra |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | luhGPX_Escorene-Ultra-LD-727-22.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Escorene Ultra LD727.22 is a high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness. |
| General Information | |
|---|---|
| Additive |
|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 3.8 | g/10 min | ASTM D1238 |
| Vinyl Acetate Content | 18.0 | wt% | ExxonMobil Method |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness | ASTM D2240 | ||
| Shaw A, 15 seconds | 92 | ASTM D2240 | |
| Shaw D, 15 seconds | 34 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength (Break) | 9.74 | MPa | ASTM D638 |
| Tensile Elongation (Break) | 1500 | % | ASTM D638 |
| Flexural Modulus - 1% Secant | 52.7 | MPa | ASTM D790 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Vicat Softening Temperature | 59.0 | °C | ASTM D1525 |
| Legal statement |
|---|
| 有关潜在食品接触应用合规信息(例如:FDA、EU、HPFB),请与埃克森美孚化工客户服务代表联系。 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RELENE® 52GB010 | Reliance Industries Limited | HDPE | RELENE® |
| SCHULAMID® 66 GF 30 HE | A. Schulman Europe | Nylon 66 | SCHULAMID® |
| SUMIPEX® MH | Sumitomo Chemical Co., Ltd. | Acrylic (PMMA) | SUMIPEX® |
| APEX® 85-J438-H | Teknor Apex Company | PVC, Flexible | APEX® |
| XYLEX™ FXY330DF resin | SABIC Innovative Plastics Europe | PC+Polyester | XYLEX™ |