Category: | PPA , Polyphthalamide |
Manufacturer: | PolyOne Corporation |
Trademark: | Edgetek™ |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | lrxv9v_Edgetek-AM-35GF-000-FR-NH.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads. |
General Information | |
---|---|
Filler / Reinforcement |
|
Features |
|
Uses |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.51 | g/cm³ | ISO 1183 |
Molding Shrinkage | ISO 294-4 | ||
Across Flow : 2.00 mm | 0.70 | % | |
Flow : 2.00 mm | 0.10 | % |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 12500 | MPa | ISO 527-2 |
Tensile Stress (Break) | 150 | MPa | ISO 527-2 |
Tensile Strain (Break) | 2.0 | % | ISO 527-2 |
Flexural Modulus | 10000 | MPa | ISO 178 |
Flexural Stress | 210 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength (23°C) | 6.0 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength (23°C) | 50 | kJ/m² | ISO 179/1eU |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Annealed) | 280 | °C | ISO 75-2/A |
Melting Temperature | 320 to 330 | °C | ISO 11357-3 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Comparative Tracking Index | 600 | V | IEC 60112 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating | UL 94 | ||
0.800 mm | V-0 | ||
1.60 mm | V-0 | ||
3.00 mm | V-0 | ||
Glow Wire Flammability Index | IEC 60695-2-12 | ||
0.800 mm | 960 | °C | |
1.60 mm | 960 | °C | |
3.00 mm | 960 | °C | |
Glow Wire Ignition Temperature | IEC 60695-2-13 | ||
0.800 mm | 750 | °C | |
1.60 mm | 750 | °C | |
3.00 mm | 775 | °C | |
Oxygen Index | > 34 | % | ISO 4589-2 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 120 | °C | |
Drying Time | 4.0 | hr | |
Suggested Max Moisture | < 0.10 | % | |
Processing (Melt) Temp | 320 to 340 | °C | |
Mold Temperature | 90.0 to 120 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 1385 TFE 15 SI 2 | RTP Company | PPS | RTP |
PONYL 4009EPG15 | POLYROCKS CHEMICAL CO., LTD | Nylon 6 | PONYL |
HiFill® PPS GF/M55 BK | Techmer Engineered Solutions | PPS | HiFill® |
Kemcor LD 0231 | Qenos Pty Ltd | LDPE | Kemcor |
K PP 7072 | Technovinyl Polymers India Ltd. | TPO | K PP |