| Category: | PUR-Ether/TDI , Polyurethane (Polyether, TDI) |
| Manufacturer: | Anderson Development Company |
| Trademark: | Andur |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | lkXVGs_Andur-9200-AP.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Andur 9200-AP is a polyether (PPG) based liquid, toluene diisocyanate terminated prepolymer. An elastomer with a hardness of 92 Shore A is obtained when this prepolymer is cured with Curene 442 [4,4'-methylene-bis (orthochloroaniline)]. Elastomers of lower hardness can be obtained by curing Andur 9200-AP with polyols and their combination with Curene 442 and other diamines, or through the use of plasticizers. |
| General Information | |
|---|---|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.09 | g/cm³ | ASTM D792 |
| Thermoset | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Thermoset Mix Viscosity | ASTM D2393 | ||
| 21°C | 21500 | cP | ASTM D2393 |
| 70°C | 800 | cP | ASTM D2393 |
| 100°C | 165 | cP | ASTM D2393 |
| Additional Information |
|---|
| NCO: 5.4 to 5.8%Specific Gravity, ASTM D792, 70°F: 1.092 g/mlSpecific Gravity, ASTM D792, 212°F: 1.062 g/ml |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Shin-Etsu RTV KE-3472T | Shin-Etsu Silicones of America | Silicone Rubber, RTV-1 | Shin-Etsu RTV |
| Tecomid® NB40 GR20 NL | Eurotec Engineering Plastics | Nylon 6 | Tecomid® |
| WELLAMID Nylon 6000 GS 50 HWUVCP | CP-Polymer-Technik GmbH & Co. KG | Nylon 6 | WELLAMID Nylon |
| XYRON™ X531V | Asahi Kasei Chemicals Corporation | PPE+PS | XYRON™ |
| EXCELLOY CW50 | Techno Polymer Co, Ltd. | AES+PC | EXCELLOY |