Glass Fiber
General Information
Filler / Reinforcement
  • Glass fiber reinforced material, 50% filler by weight
RoHS Compliance
  • Contact manufacturer
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.62g/cm³ASTM D792
Molding Shrinkage - Flow (3.20 mm)0.20 - 0.30%ASTM D955
Water Absorption (23°C, 24 hr)0.20%ASTM D570
Moisture Content 0.10%
Additional InformationNominal ValueUnit
Primary Additive 50%
HardnessNominal ValueUnitTest Method
Rockwell Hardness (R-Scale)125ASTM D785
MechanicalNominal ValueUnitTest Method
Tensile Modulus 16500MPaASTM D638
Tensile Strength 234MPaASTM D638
Tensile Elongation (Yield)1.5 - 3.0%ASTM D638
Flexural Modulus 17200MPaASTM D790
Flexural Strength 359MPaASTM D790
ImpactNominal ValueUnitTest Method
Notched Izod Impact (3.20 mm)120J/mASTM D256
Unnotched Izod Impact (3.20 mm)910J/mASTM D4812
ThermalNominal ValueUnitTest Method
Deflection Temperature Under Load (1.8 MPa, Unannealed)279°CASTM D648
ElectricalNominal ValueUnitTest Method
Volume Resistivity > 1.0E+15ohms·cmASTM D257
FlammabilityNominal ValueUnitTest Method
Flame Rating (1.50 mm, ** Values per RTP Company testing.)HBUL 94
InjectionNominal ValueUnit
Drying Temperature 107°C
Drying Time 4.0 - 6.0hr
Dew Point -28.9°C
Processing (Melt) Temp 329 - 343°C
Mold Temperature 65.6 - 163°C
Injection Pressure 68.9 - 103MPa
Injection instructions
Desiccant Type Dryer Required.
Resin Grade Manufacturer Category Trademark
RTP 200 UV RTP Company Nylon 66 RTP
RTP 2387 C RTP Company PUR, Unspecified RTP
Rhelon G3533H-01 RheTech, Inc. Nylon 66/6 Rhelon
FRAGOM PR/04 AFKK N Crosspolimeri S.p.A. TP, Unspecified FRAGOM
Petrothene® GA601 LyondellBasell Industries LLDPE Petrothene®