Rilsan® AMN G8 TLD is a Polyamide 12 (Nylon 12) product filled with filler. It can be processed by injection molding and is available in Africa & Middle East, Asia Pacific, Europe, Latin America, or North America. Characteristics include:
|
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Forms |
|
Processing Method |
|
Multi-Point Data |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1020 | 1020 | kg/m³ | ISO 1183 1 |
Melt volume-flow rate (235°C/2.16 kg) | 61.0 | -- | cm³/10min | ISO 1133 2 |
Water Absorption (Saturation) | 1.6 | -- | % | ISO 62 3 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile modulus | 1520 | 1360 | MPa | ISO 527-2 4 |
Tensile Stress (Yield) | 45.0 | 39.0 | MPa | ISO 527-2 5 |
Tensile Strain (Yield) | 10 | 12 | % | ISO 527-2 6 |
Nominal strain at break | > 50 | > 50 | % | ISO 527-2 7 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy notched impact strength | ISO 179/1eA 8 | |||
-30°C | 4.00 | 4.00 | kJ/m² | |
23°C | 4.00 | 5.00 | kJ/m² | |
Charpy impact strength | ISO 179/1eU 9 | |||
-30°C | No Break | No Break | ||
23°C | No Break | No Break |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Deflection Temperature Under Load | ISO 75-2 10 | |||
0.45 MPa | 143 | -- | °C | |
1.8 MPa | 65.0 | -- | °C | |
Vicat Softening Temperature (50°C/h, B (50N)) | 145 | -- | °C | ISO 306 11 |
Melting Temperature 12 | 178 | -- | °C | ISO 11357-3 13 |
CLTE - Flow | 8.0E-5 | -- | cm/cm/°C | ISO 11359-2 14 |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Surface resistivity | -- | 1.0E+14 | ohms | IEC 60093 15 |
Volume resistivity | -- | 1.0E+12 | ohms·m | IEC 60093 16 |
Relative Permittivity | IEC 60250 17 | |||
100 Hz | 5.00 | -- | ||
1 MHz | 3.00 | -- | ||
Dissipation Factor | IEC 60250 18 | |||
100 Hz | 0.094 | -- | ||
1 MHz | 0.036 | -- | ||
Comparative tracking index | -- | 600 | IEC 60112 19 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Burning Behav. at 1.6mm nom. thickn. (1.60 mm) | HB | -- | ISO 1210 20 | |
Burning Behav. at thickness h (3.20 mm) | HB | -- | ISO 1210 21 | |
Oxygen index | 22 | -- | % | ISO 4589-2 22 |
Note Message | |
---|---|
1 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
2 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
3 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
4 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
5 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
6 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
7 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
8 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
9 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
10 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
11 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
12 . | 10 °C/min |
13 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
14 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
15 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
16 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
17 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
18 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
19 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
20 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
21 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
22 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
AKROMID® B3 GF 40 9 RM-M natural (3414) | AKRO-PLASTIC GmbH | Nylon 6 | AKROMID® |
Cheng Yu PP237G2 | Cheng Yu Plastic Company Limited | PP, Unspecified | Cheng Yu |
HIVOREX 6200B | Lotte Chemical Corporation | HDPE | HIVOREX |
Huafon JF-P-4170T / JF-I-4118 (outsole) | Huafon Group Co., Ltd. | PUR-Ester | Huafon |
Sylvin 2900-78 Clear | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |