| Category: | TPE , Thermoplastic Elastomer |
| Manufacturer: | Mitsubishi Chemical Performance Polymers, Inc. |
| Trademark: | THERMORUN® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | lU7Lse_THERMORUN-3707N.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| THERMORUN®3707N is a thermoplastic elastomer (TPE) material,. This product is available in North America, Europe or Asia Pacific. The processing method is extrusion. THERMORUN®The main characteristics of 3707N are: low hardness. |
| General Information | |
|---|---|
| Features |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.880 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (230°C/5.0 kg) | 3.0 | g/10 min | ISO 1133 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A) | 68 | ISO 868 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ISO 37 | ||
| 100% strain | 2.30 | MPa | ISO 37 |
| 300% strain | 3.50 | MPa | ISO 37 |
| Tensile Stress (Break) | 7.00 | MPa | ISO 37 |
| Tensile Elongation (Break) | 600 | % | ISO 37 |
| Tear Strength | 40 | kN/m | ISO 34-1 |
| Compression Set (70°C, 22 hr) | 43 | % | ISO 815 |
| Additional Information |
|---|
| Data obtained using JIS test methods. |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Maxelast® A9810 | Nantong Polymax Elastomer Technology, Co., Ltd | TPE | Maxelast® |
| Salflex 635GC | Salflex Polymers Ltd. | PP Copolymer | Salflex |
| Bionate® 55D | DSM Biomedical Inc. | PC+TPU | Bionate® |
| EXCELLOY CK55 | Techno Polymer Co, Ltd. | PC+ABS | EXCELLOY |
| Huafon JF-D-C8903 | Huafon Group Co., Ltd. | PUR, Unspecified | Huafon |