| Category: | PC , Polycarbonate |
| Manufacturer: | Ginar Technology Co., LTD. |
| Trademark: | Kapex |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | lMU0zG_Kapex-C322.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| 10% Glass reinforced |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.27 | g/cm³ | ASTM D792 |
| Molding Shrinkage - Flow (1.60 mm) | 0.50 | % | ASTM D955 |
| Water Absorption (24 hr) | 0.050 | % | ASTM D570 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Rockwell Hardness (R-Scale) | 120 | ASTM D785 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength (Yield) | 82.7 | MPa | ASTM D638 |
| Tensile Elongation (Break) | 4.5 | % | ASTM D638 |
| Flexural Modulus | 3790 | MPa | ASTM D790 |
| Flexural Strength | 145 | MPa | ASTM D790 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact (23°C) | 120 | J/m | ASTM D256 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Deflection Temperature Under Load (1.8 MPa, Unannealed) | 140 | °C | ASTM D648 |
| Flammability | Nominal Value | Test Method | |
|---|---|---|---|
| Flame Rating | UL 94 | ||
| 0.794 mm | HB | ||
| 1.59 mm | HB | ||
| 3.18 mm | HB |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| SureSpec PET-80HF | Genesis Polymers | PET | SureSpec |
| DOWLEX™ 4056G | The Dow Chemical Company | LLDPE | DOWLEX™ |
| Elastollan® 1185AF001 | BASF Corp. Thermoplastic Polyurethanes | TPU-Polyether | Elastollan® |
| HIFOR Xtreme® SC74869 | Westlake Chemical Corporation | LLDPE | HIFOR Xtreme® |
| RONFALIN® ABS 1328 | A. Schulman Europe | ABS | RONFALIN® |