Category: | PBT , Polybutylene Terephthalate |
Manufacturer: | Polykemi AB |
Trademark: | POLYshine |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | lDwZ8g_POLYshine-PBT-D221-GF30.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Glass fibre-reinforced |
General Information | |
---|---|
Filler / Reinforcement |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.49 | g/cm³ | ISO 1183 |
Molding Shrinkage | ISO 294-4 | ||
Across Flow | 1.2 | % | |
Flow | 0.30 | % |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | 140 | MPa | ISO 527-2 |
Tensile Strain (Break) | 2.5 | % | ISO 527-2 |
Flexural Modulus (23°C) | 7700 | MPa | ISO 178 |
Flexural Stress | 175 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179 | ||
-20°C | 7.0 | kJ/m² | |
23°C | 8.0 | kJ/m² |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature 1 | |||
0.45 MPa, Unannealed | 220 | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 210 | °C | ISO 75-2/A |
Vicat Softening Temperature | 215 | °C | ISO 306/B50 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating (1.60 mm) | HB | UL 94 | |
Glow Wire Ignition Temperature (2.00 mm) | 750 | °C | IEC 60695-2-13 |
Note Message | |
---|---|
1 . | 120°C/hr |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Jam HDPE HM9450F1 | Jam Petrochemical Company | HDPE | Jam HDPE |
LubriOne™ NN-30CF/15T-02S black | PolyOne Corporation | Nylon 66 | LubriOne™ |
Magnobond 6289 | Magnolia Plastics, Inc. | Epoxy | Magnobond |
Sylvin 8344-75 Black | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
Sylvin 7833-60 Red 604 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |