Wellamid® 42L XE-N is a Polyamide 6 (Nylon 6) material. It is available in Asia Pacific, Europe, Latin America, or North America for injection molding.

Typical applications include:
  • Automotive
  • Engineering/Industrial Parts
General Information
Uses
  • Engineered Applications
Forms
  • Pellets
Processing Method
  • Injection Molding
PhysicalNominal ValueUnitTest Method
Density 1.13g/cm³ISO 1183
Molding Shrinkage ISO 294-4
    Across Flow : 23°C 1.2 to 1.6%
    Flow : 23°C 1.2 to 1.6%
MechanicalNominal ValueUnitTest Method
Tensile Stress (Yield, 23°C)75.0MPaISO 527-2
Tensile Strain (Yield, 23°C)65%ISO 527-2
Flexural Modulus (23°C)2600MPaISO 178
Flexural Stress (23°C)100MPaISO 178
ImpactNominal ValueUnitTest Method
Notched Izod Impact Strength (23°C)6.0kJ/m²ISO 180
ThermalNominal ValueUnitTest Method
Heat Deflection Temperature (1.8 MPa, Unannealed)55.0°CISO 75-2/A
Melting Temperature (DSC) 220°CISO 3146
InjectionNominal ValueUnit
Drying Temperature 79.4°C
Drying Time 2.0 to 4.0hr
Suggested Max Moisture 0.20%
Rear Temperature 238 to 282°C
Middle Temperature 232 to 277°C
Front Temperature 227 to 271°C
Nozzle Temperature 227 to 293°C
Processing (Melt) Temp 227 to 293°C
Mold Temperature 71.1 to 93.3°C
Injection Pressure 34.5 to 138MPa
Back Pressure 0.345MPa
Screw Speed 30 to 120rpm
Resin Grade Manufacturer Category Trademark
RTP 4103 RTP Company PEKK RTP
Gallonprene® GP420-3003 Shenzhen Sungallon Rubber & Plastic Corporation Limited TPE Gallonprene®
ESTADIENE 0615 HHT Cossa Polimeri S.r.l. ABS ESTADIENE
LNP™ THERMOCOMP™ HF006EU compound SABIC Innovative Plastics Europe Nylon 11 LNP™ THERMOCOMP™
CYCOLOY™ C2950HF resin SABIC Innovative Plastics PC+ABS CYCOLOY™