Category: | TPV , Thermoplastic Vulcanizate |
Manufacturer: | Teknor Apex Company |
Trademark: | Sarlink® TPV |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | kogMlk_Sarlink-TPV-2645.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Sarlink®TPV 2645 is a thermoplastic vulcanized rubber (TPV) material,. This product is available in North America, Africa and the Middle East, Latin America, Europe or Asia Pacific. The processing method is extrusion or injection molding. Typical application areas include:
|
General Information | |
---|---|
Uses |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 0.910 | g/cm³ | ASTM D792 |
Melt Mass-Flow Rate (MFR) (235°C/2.16 kg) | 1.5 | g/10 min | ASTM D1238 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A, 5 sec) | 51 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (100% Strain) | 1.72 | MPa | ASTM D412 |
Tensile Strength 1(Break, 23°C) | 3.45 | MPa | ASTM D412 |
Tensile Elongation (Break) | 300 | % | ASTM D412 |
Tear Strength | 14.2 | kN/m | ASTM D624 |
Compression Set | ASTM D395 | ||
23°C, 22 hr | 15 | % | ASTM D395 |
70°C, 22 hr | 32 | % | ASTM D395 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Brittleness Temperature 2 | > -60.0 | °C | ASTM D746 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Rear Temperature | 173 - 213 | °C | |
Middle Temperature | 179 - 219 | °C | |
Front Temperature | 184 - 224 | °C | |
Nozzle Temperature | 190 - 230 | °C | |
Processing (Melt) Temp | 190 - 230 | °C | |
Mold Temperature | 35.0 - 60.0 | °C | |
Injection Pressure | 1.38 - 6.89 | MPa | |
Injection Rate | Fast | ||
Back Pressure | 0.172 - 0.862 | MPa | |
Screw Speed | 50 - 120 | rpm | |
Cushion | 3.81 - 25.4 | mm |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Cylinder Zone 1 Temp. | 166 - 204 | °C | |
Cylinder Zone 2 Temp. | 171 - 210 | °C | |
Cylinder Zone 3 Temp. | 177 - 216 | °C | |
Cylinder Zone 5 Temp. | 182 - 221 | °C | |
Die Temperature | 190 - 227 | °C |
Extrusion instructions |
---|
Screw Speed: 30 to 100 rpm |
Note Message | |
---|---|
1 . | 510 mm/min |
2 . | No Break @ -76°F. |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
NILENE® P | Taro Plast S.p.A. | PP Homopolymer | NILENE® |
Chemraz 514 | Greene, Tweed & Co. | Perfluoroelastomer | Chemraz |
EnCom PC-PBT 1174SP | EnCom, Inc. | PC+PBT | EnCom |
PermaStat® 1200 | RTP Company | TPU-Polyester | PermaStat® |
KOPA® KN333G50 | Kolon Plastics, Inc. | Nylon 66 | KOPA® |