RTP ESD A 2800-85A

Category: TPO (POE) , Thermoplastic Polyolefin Elastomer
Manufacturer: RTP Company
Trademark: RTP
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: kgRnGk_RTP-ESD-A-2800-85A.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Warning: The status of this material is 'Commercial: Limited Issue'

The data for this material has not been recently verified.
Please contact RTP Company for current information prior to specifying this grade.

Static Dissipative - 85 Shore A
General Information
Features
  • Electrostatic discharge protection
  • Static conduction
RoHS Compliance
  • Contact manufacturer
Forms
  • Particle
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.01g/cm³ASTM D792
Molding Shrinkage - Flow (3.20 mm)1.6 - 2.0%ASTM D955
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shore A, 10 sec)85ASTM D2240
ElastomersNominal ValueUnitTest Method
Tensile Strength (Yield)9.65MPaASTM D412
Tensile Elongation (Yield)500%ASTM D412
ElectricalNominal ValueUnitTest Method
Surface Resistivity 5.0E+5ohmsASTM D257
Volume Resistivity 5.0E+4ohms·cmASTM D257
Additional Information
Dew Point: 0°FMoisture Content: 0.03%Static Decay, FTMS101C, 4046.1, MIL-PRF-81705D, 50V to 5kV, 12%RH: <2 sSurface Resistivity, ASTM D257: 1000000 to 9.9E+12 ohmSurface Resistivity, ESD S11.11: 100000 to 9.9E+11 ohmTensile Elongation, ASTM D412: >500%Volume Resistivity, ASTM D257: 1000 to 9900000000 ohm-cm
InjectionNominal ValueUnit
Drying Temperature 79.4°C
Drying Time 2.0hr
Processing (Melt) Temp 182 - 210°C
Mold Temperature 15.6 - 65.6°C
Injection Pressure 82.7 - 124MPa
Resin Grade Manufacturer Category Trademark
Salflex 375AH Salflex Polymers Ltd. TPV Salflex
TechnoDur PBT 4 GF30 FR TechnoCompound GmbH PBT TechnoDur
ELITE™ 5101G The Dow Chemical Company EPE ELITE™
Electrafil® PA6/6 03005 CF Techmer Engineered Solutions Nylon 66 Electrafil®
PC-COM™ PC415 Polymer Compounders Limited PC PC-COM™