| Category: | Nylon 66 , Polyamide 66 |
| Manufacturer: | Politem Plastik Ltd. |
| Trademark: | PAmpellonne® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | kEt80g_PAmpellonne-rgr-wss.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| All Politem Plastik Polyamide Resins are recycled from Post Industrial Fiber Waste Streams |
| General Information | |
|---|---|
| Recycled Content |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.13 to 1.15 | g/cm³ | ISO 1183 |
| Ash Content | 0.30 to 0.80 | % | ISO 3451-4 |
| Moisture | 0.10 to 0.70 | % | ISO 15512/B |
| Relative Viscosity 1 | 2.40 to 2.50 |
| Additional Information | Nominal Value | Unit | |
|---|---|---|---|
| DSC Analysis | > 95 | % |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Shore Hardness (Shore D) | 85 to 100 | ISO 868 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 2500 to 4000 | MPa | ISO 527-2 |
| Tensile Stress (Yield) | 50.0 to 90.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | > 3.0 | % | ISO 527-2 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | 5.0 to 6.0 | kJ/m² | ISO 179/1A |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Melting Temperature (DSC) | 263 to 271 | °C | ISO 3146 |
| Note Message | |
|---|---|
| 1 . | Formic |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| PRIMALLOY® A1900 | Mitsubishi Chemical Performance Polymers, Inc. | TPE | PRIMALLOY® |
| ALCOM® PA66 910/1.1 CF10 GF10 IM | ALBIS PLASTIC GmbH | Nylon 66 | ALCOM® PA66 |
| Bormed™ BE860MO | Borealis AG | PP Copolymer | Bormed™ |
| Karina BLACK PVC COMPOUND 834-48/ 1-A-ERM-LMP | Karina Ind. e Com. de Plásticos Ltda | PVC, Unspecified | Karina |
| Durez® 34127 | SBHPP | Phenolic | Durez® |