Category: | PUR-Ester/TDI , Polyurethane (Polyester, TDI) |
Manufacturer: | Anderson Development Company |
Trademark: | Andur |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | k6tocd_Andur-8-APF-LM-Curene-3005.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
All properties based on Andur® 8-APF-LM cured with Curene® 3005 |
General Information | |
---|---|
Forms |
|
Processing Method |
|
Hardness | Nominal Value | Test Method | |
---|---|---|---|
Durometer Hardness (Shore A) | 72 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | 31.8 | MPa | ASTM D638 |
Tensile Elongation (Break) | 760 | % | ASTM D638 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | ASTM D412 | ||
100% strain | 2.86 | MPa | ASTM D412 |
300% strain | 4.00 | MPa | ASTM D412 |
Tear Strength | |||
-- 1 | 43.8 | kN/m | ASTM D624 |
Cracking | 25 | kN/m | ASTM D470 |
Compression Set | 42 | % | ASTM D395 |
Thermoset | Nominal Value | Unit | |
---|---|---|---|
Pot Life | 9.0 - 11 | min | |
Demold Time | 60 | min | |
Post Cure Time (23°C) | 72 | hr |
Additional Information |
---|
Prepolymer NCO%: 2.9-3.3Grams Curene® 3005 per 100 grams prepolymer: 20.3Rebound, %: 43Stoichiometry: 0.95Prepolymer Temperature, °F: 190-210Curene® 3005 Temperature, °F: 158Post Cure Time, 212°F, hours: 16 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Mold Temperature | 107 | °C |
Note Message | |
---|---|
1 . | C mould |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 307 UV | RTP Company | PC | RTP |
Sofprene T® 550100A70 | SO.F.TER. SPA | SBS | Sofprene T® |
ALCUDIA® LDPE PE-015 | REPSOL | LDPE | ALCUDIA® LDPE |
HI-ZEX™ 7000F | Prime Polymer Co., Ltd. | HDPE | HI-ZEX™ |
LUVOCOM® 1-8068/GN | Lehmann & Voss & Co. | Nylon 66 | LUVOCOM® |