Polyamide 66, %50 glass fiber reinforced
General Information
Filler / Reinforcement
  • Glass Fiber
PhysicalNominal ValueUnitTest Method
Density 1.42 to 1.50g/cm³ISO 1183
Molding Shrinkage 0.15 to 0.20%
HardnessNominal ValueUnitTest Method
Shore Hardness (Shore D)75 to 85ISO 868
MechanicalNominal ValueUnitTest Method
Tensile Modulus 10000 to 13000MPaISO 527-2
Tensile Stress (Yield)190 to 230MPaISO 527-2
Tensile Strain (Break)> 3.0%ISO 527-2
ImpactNominal ValueUnitTest Method
Notched Izod Impact Strength > 7.0kJ/m²ISO 180/1A
ThermalNominal ValueUnitTest Method
Heat Deflection Temperature (1.8 MPa, Unannealed)250°CISO 75-2/A
Vicat Softening Temperature 255°CISO 306/B
Melting Temperature (DSC) 265°CISO 3146
Resin Grade Manufacturer Category Trademark
Menzolit® BMC 2310 Menzolit Ltd (UK) Polyester, TS Menzolit®
TECHNO ABS F5451G30 Techno Polymer Co, Ltd. ABS TECHNO ABS
SNOLEN® EF 0.21/46 HT JSC Gazprom neftekhim Salavat HDPE SNOLEN®
Catalyst CT/2-LR Solvay Specialty Polymers Polyolefin, Unspecified Catalyst
Eastar™ MN052 Eastman Chemical Company Copolyester Eastar™